| MAGNETIC PROPERTIES AND STRUCTURE OF ULTRAFINE (um ORDER) Fe-Cu-Mo-Si-B ALLOY |
| TU Guochao;ZHANG Jiaji;JI Yu;SHI Changli Institute of Metallurgy; Shoudou Iron and Steel Company; Beijing |
|
Cite this article:
TU Guochao;ZHANG Jiaji;JI Yu;SHI Changli Institute of Metallurgy; Shoudou Iron and Steel Company; Beijing. MAGNETIC PROPERTIES AND STRUCTURE OF ULTRAFINE (um ORDER) Fe-Cu-Mo-Si-B ALLOY. Acta Metall Sin, 1991, 27(3): 154-156.
|
|
|
Abstract The variation of magnetic properties with different regimes of magnetic anneal-ing and temperatures of heat treatment has been investigated on the ultrafine (nm order) softmagnetic material of Fe_(84.32)Cu_(1.06)Mo_(5.78)Si_(7.2)B_(1.64)(wt-%) alloy, prepared by annealing amorphousstate and single rolling over its crystallization temperature. A optimum performance with agingat 510℃ for 1h then slow cooling was found. The structural observation under TEM toge-ther with X-ray diffraction and thermomagnetic analysis were determined that the alloy iscomposed of two phases, i. e. a-FeSi solid solution about size 10--20 nm, and amorphousphase.
|
|
Received: 18 March 1991
|
1 山内清隆技术,1988;8(12) ;46 2 Herzer G. IEEE Trans Magn, 1989; MAG-25: 3327 3 Yoshizawa Y, Oguma S, Yamachi K. J Appl Phys, 1988; 64: 6044 4 吉沢克仁,山内清隆.日本金属学会志,1989;53:241 5 Yoshizawa Y, Yamauchi K. IEEE Trans Magn. 1989; MAG-25: 3324T |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|