EFFECT OF EXPLOSIVE CONSOLIDATION PARAMETERS ON CONSOLIDATION QUALITY
GAO Juxian;ZHANG Ke;ZHENG Zhemin Institute of Mechanics; Academia Sinica; Beijing
Cite this article: 

GAO Juxian;ZHANG Ke;ZHENG Zhemin Institute of Mechanics; Academia Sinica; Beijing. EFFECT OF EXPLOSIVE CONSOLIDATION PARAMETERS ON CONSOLIDATION QUALITY. Acta Metall Sin, 1990, 26(6): 159-161.

Download:  PDF(261KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Two-dimension consolidation under the cylindrical converging shock wave hasbeen studied. The major parameters influenced on the explosive consolidation quality are thespecific energy, detonation pressure and specific impulse. It seems to be favourable to impro-ving consolidation quality by a lower but slightly higher than critical detonation pressure and ahigh specific impulse.
Key words:  explosive consolidation      shock wave      explosive parameter     
Received:  18 June 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I6/159

1 高举贤,邵丙璜,张科,郑哲敏.金属学报,1990;26:B349
2 高举贤,王晓林,张晓红,中国科学院力学研究所内部资料,1990
[1] FENG Aixin NIE Guifeng XUE Wei CAO Yupeng XU Xiaoxiang LI Bin SHI Fen . EXPERIMENTAL RESEARCH ON LASER SHOCK WAVE LOADING MECHANISM OF 2024 ALUMINUM ALLOY SHEET[J]. 金属学报, 2012, 48(2): 205-210.
[2] LIU Zuoquan; ZHAO Heyun; LU Yusong; LI Dexiu; LI Hin; ZHANG Shubo (Yunnan Univereity; Kunming 650091)(Manuscript received 1995-11-13; in revised form 1996-04-04). CRYSTALLIZATION OF AMORPHOUS ALLOY Fe_(78)B_(13)Si_9 INDUCED BY SHOCK WAVE[J]. 金属学报, 1996, 32(8): 862-866.
[3] CHEN Liangshan; ZHAO Tiemin ;SI Zhongyao (Institute of Metal Research;Chinese Academy of Sciences; Shenyang)(Manuscript received 18 November;1993; in revised form 21 January;1994). EFFECT OF REFLECTED TENSION SHOCK WAVE ON MICROSTRUCTURE AND FATIGUE PROPERTY OF 16Mn STEEL WELD[J]. 金属学报, 1994, 30(23): 519-523.
[4] ZHAO Tiemin;CHEN Liangshan;SI Zhongyao(Institute of Metal Research;Chinese Academy of Scicnces; Shenyang);TAN Shengyu;CUI Guangyuan (ShenyangInstitute of Artillery). EFFECT OF EXPLOSION SHOCK WAVE INTENSITY ON DISLOCATION STRUCTURE IN FERRITE OF STEEL 16Mn WELD[J]. 金属学报, 1994, 30(15): 130-135.
[5] CHEN Liangshan;SI Zhongyao;TAN Shengyu;CUI Guangyuan Institute of Metal Research; Academia Sinica; Shenyang Shenyang Institute of AritilleryCHEN Huaining;research associate;Institute of Metal Research Academia Sinica;Shenyang 110015. REDUCTION OF da/dN AT DIFFERENT SHOCK WAVE AFFECTING REGIONS[J]. 金属学报, 1993, 29(6): 38-42.
[6] GAO Juxian;SHAO Binghuang;ZHANG Ke;ZHENG Zhemin Institute of Mechanics; Academia Sinica; Beijing. EXPLOSIVE CONSOLIDATION OF METAL UNDER CYLINDRICAL CONVERGING SHOCK WAVE[J]. 金属学报, 1990, 26(5): 125-130.
No Suggested Reading articles found!