Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (6): 110-116    DOI:
Current Issue | Archive | Adv Search |
CHANGE OF ECCENTRICITY IN TUBE SINKING
YAO Ruohao;ZHONG Jianhua;HUANG Jianfang;ZHANG Ruhua South Institute of Metallurgy; Ganzhou; Jiangxi
Cite this article: 

YAO Ruohao;ZHONG Jianhua;HUANG Jianfang;ZHANG Ruhua South Institute of Metallurgy; Ganzhou; Jiangxi. CHANGE OF ECCENTRICITY IN TUBE SINKING. Acta Metall Sin, 1990, 26(6): 110-116.

Download:  PDF(521KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The rectification of eccentricity was revealed to be more effective intube sinking than drawing wan a mandral. The ratio of thickness to diameter oftube blank on both sides of thick and thin wall seems to be the principal influen-tial factor in rectifying eccentricity. The greater the initial outside diameter and theinitial wall thickness difference are and the less the initial wall thickness of thetube blank is, the better the rectification.
Key words:  sinking tube      eccentricity      rectifying     
Received:  18 June 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I6/110

1 姚若浩,钟建华,刘小林,莫建平.金属学报,1986;22:B116
2 田中浩,佐藤优,吉田一也.伸铜技术研究会志,1978;17:189
3 田中浩,佐藤优,吉田一也.伸铜技术研究会志,1979;18:209
4 田中浩,佐藤优,吉田一也.伸铜技术研究会志,1986;25:29
5 杨守山.有色金属塑性加工学.北京:冶金工业出版社,1982:307
6 Безухов Н И,杜庆华译.弹性与塑性理论,北京:人民教育出版社,1963:185
7 #12
8 #12
9 田中浩,佐藤优,吉田一也.伸铜技术研究会志,1981;20:230
No related articles found!
No Suggested Reading articles found!