CALCULATION OF THERMODYNAMIC PROPERTIES OF In-Bi-Tl TERNARY ALLOYS
Cite this article: 

CALCULATION OF THERMODYNAMIC PROPERTIES OF In-Bi-Tl TERNARY ALLOYS. 0412-1961. Acta Metall Sin, 1990, 26(4): 108-112.

Download:  PDF(360KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  ZHENG Minhui;KOZUKA Zensaku University of Science and Technology Beijing Faculty of Engineering, Osaka University Department of Physical Chemistry,University of Science and Technology Beijing, Beijing 100083
Key words:  Acta Metallurgica Sinica<1990.04>     
Received:  18 April 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I4/108

1 Yao S, Zheng M, Kozuka Z. J Less-Common Met, 1987; 128: 213
2 郑敏辉,幸塚善作,日本金属学会志,1986;50:804
3 郑敏辉,幸塚善作,日本金属学会志,1987;51:44
4 Zheng M, Kozuka Z. Trans Jpn Inst Met, 1987; 28: 925
5 郑敏辉,幸塚善作.日本金属学会志,1987;51:666
6 片山巌,柴田纯,幸塚善作.日本金属学会志,1975;39:990
7 Hultgren R, Desai P D, Hawkins D T, Gleiser M, Kelley K K. Selected Values of Thermodynamic Properties of Binary Alloys, Metals Park, Ohio: ASM, 1973
8 Darken L S. J Am Chem Soc, 1950; 72: 2909
9 Hoshino H, Nakamura Y, Shimoji M, Niwa K. Ber Bunsenges, 1965; 69: 414
10 Lamparter P, Cocke D L, Steele S. Z Metallk, 1982; 73: 149%
No related articles found!
No Suggested Reading articles found!