Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (2): 16-20    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF NITROGEN ON MICROSTRUCTURE AND PROPERTIES OF HK50 ALLOY
YU Yongsi;CAO Zhiben;WANG Fugang;GUO Xiaobing Dalian University of Technology Jinzhou Institute of Technology lecturer;Department of Materials Engineering;Dalian University of Technology; Dalian 116024
Cite this article: 

YU Yongsi;CAO Zhiben;WANG Fugang;GUO Xiaobing Dalian University of Technology Jinzhou Institute of Technology lecturer;Department of Materials Engineering;Dalian University of Technology; Dalian 116024. EFFECT OF NITROGEN ON MICROSTRUCTURE AND PROPERTIES OF HK50 ALLOY. Acta Metall Sin, 1990, 26(2): 16-20.

Download:  PDF(752KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The volume fraction of the larmellar cell in HK50 alloy may beincreased with the increase of N_2 content over 0.065%. The habit plane of larme-llar carbide is {111}_γ. The distribution of N_2 changes no more before or after thelarmellar cell precipitated. The diffusion activation energy of carbon reducesremarkably with the increase of N_2 content. It is believed that the larmellar carbi-de is harmful to the high temperature creep and impact properties of the alloy.
Key words:  HK50 alloy      larmellar carbide      habit plane      diffusion activation energy     
Received:  18 February 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I2/16

1 石子源,于永泗,曹智本,王焕庭.金属热处理,1986;(12) :33
2 高温合金(冶金学和生产)编辑组.高温合金(冶金学和生产),上海:科学技术文献出版社,1980:174
3 Pak H-R, Chang S N, Kato M. J Mater Sci, 1985; 20: 947
4 西野知良,国外金属材料,1975;(3) :34'
[1] GU Xinfu ZHANG Wenzheng. A SIMPLE VECTOR ANALYSIS METHOD FOR MARTENSITE CRYSTALLOGRAPHY[J]. 金属学报, 2011, 47(2): 241-245.
[2] Dong Qiu; Wenzheng Zhang. Research Progress in Precipitation Crystallography models[J]. 金属学报, 2006, 42(4): 341-349 .
[3] LUO Chengping;XU Linkang;CHA Jianzhong South-China University of Technology; Guangzhou Guangdong Iron and Steel Research InstituteDepartment of Mechanical Engineering(Ⅱ);South-China University of Technology; Guangzhou 510641. CRYSTALLOGRAPGY OF LATH MARTENSITE IN ULTRAHIGH-STRENGTH STEEL 300M[J]. 金属学报, 1993, 29(7): 28-33.
[4] GU Nanju;WANG Ruixiang;YIN Fuxing Hebei Institute of Technology; Tianjin. EFFECT OF SELF-ACCOMMODATION FOR TWINNED MARTENSITE AND INVARIANT HABIT PLANE[J]. 金属学报, 1991, 27(3): 33-40.
[5] LUO Chengping;ZHAO Fang South China University of Technology; Guangzhou. MORPHOLOGY AND CRYSTALLOGRAPHY OF ALLOY NITRIDES IN DIFFUSIONAL NITRIDED LAYER OF 4Cr5MoVlSi STEEL[J]. 金属学报, 1990, 26(6): 34-39.
[6] LIU Yumen;WU Shanghua Xi'an Jiaotong University. CHARACTERISTICS OF MARTENSITE IN A HIGH-CARBON FERROALLOY[J]. 金属学报, 1988, 24(5): 325-330.
No Suggested Reading articles found!