Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (3): 107-112    DOI:
Current Issue | Archive | Adv Search |
MICROSTRUCTURE AND MECHANICAL PROPERTIES OF TiB_2-B_4C CERAMIC COMPOSITES
LIANG Minxian;XIA Fei Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

LIANG Minxian;XIA Fei Institute of Metal Research; Academia Sinica; Shenyang. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF TiB_2-B_4C CERAMIC COMPOSITES. Acta Metall Sin, 1989, 25(3): 107-112.

Download:  PDF(2196KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The fracture strength and hardness of TiB_2 materials increase by addi-tion of 20--30 wt-% B_4C and the fracture toughness still remains on the original highlevel. The mechanism of reinforcement and crack propagation have been discussed
Key words:  TiB_2-B_4C composites      crack deflection      crack branch     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/107

1 樱井良文,小泉光惠等编,陈俊彦,王余君译.新型陶瓷(材料及其应用),北京:中国建筑工业出版社,1983:241
2 Jeffery J R, Wolff C F, Williams W S. J Am Ceram Soc, 1985; 68 (3) : C78
3 Ferber M K, Becher P F, Finch C B. J Am Cerarn Soc, 1983; 66 (1) : C2
4 Evans A G, Fu Y. In: Evans A G ed, Fracture in Ceramic Materials. New Jersey: Noyes Publications, 1984: 154
5 Baumgartuer H R, Sterger R A. J Am Ceram Soc, 1984; 67 (3) : 207C
[1] ZHAO Fangxin;ZHANG Yingjie;ZHANG Song;ZHAO Zuxin;YIN Shaokui;LI Decheng(Shenyang Research Institute of Foundry;Ministry of Machine Building Industries;Shenyang 110021)(Shenyang Polytechnic University;Shenyang 110023)(Northeastern University;Shenyang 110006)(Shenyang Research Institute of Foundry;Ministry of Machine Building Industries;Shenyang 110021)(Manuscript received 1996-02-05;in revised form 1996-05-06). FATIGUE CRACK DEFLECTION AND FORMATION OF MICROCRACKS IN POROSITY AREA OF ZG42CrMo[J]. 金属学报, 1996, 32(10): 1056-1062.
No Suggested Reading articles found!