Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (3): 102-106    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF PREPARATION CONDITION ON THERMAL EXPANSION ANISOTROPY FOR AMORPHOUS Fe_(78)B_(13)Si_9 ALLOY
LU Jian;WANG Jingtang;DING Bingzhe Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

LU Jian;WANG Jingtang;DING Bingzhe Institute of Metal Research; Academia Sinica; Shenyang. EFFECT OF PREPARATION CONDITION ON THERMAL EXPANSION ANISOTROPY FOR AMORPHOUS Fe_(78)B_(13)Si_9 ALLOY. Acta Metall Sin, 1989, 25(3): 102-106.

Download:  PDF(448KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The thermal expansion anisotropy appears in all specimens preparedunder various forming conditions. The expansion along the longitudinal direction isless than that along the transverse direction. The cooling rate, the temperature of meltbefore jet casting and the cycling temperature affect the thermal expansion coeffi-cients and anisotropy. The anisotropy of thermal expansion originates from the direc-tional atomic interaction force, atomic oscillatory frequency and the directional shortrange order structure or defects in the alloy
Key words:  amorphous Fe_(78)B_(13)Si_9 alloy      thermal expansion anisotropy     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/102

1 Kraus L, Tomas I, Kratochvilova E, Springmann B, Muller E. Phys Status Solidi (a), 1987; 100: 289
2 Zaveta K, Schneider J, Springmann B. Czech J Phys, 1985: B35: 289
3 Luborsky F E, Becker J J, McCary R O. IEEE Trans Magn, 1975; MAG11: 1644
4 Fujimori H. Obi Y, Masumoto T, Saito H. Mater Sci Eng, 1976; 23: 281
5 Morita H, Fujimori H, Obi Y. Appl Phys, 1979; 20: 125
6 E du Tremolet de Lacheisserie. J Magn Magn Mater, 1987; 66: 102
7 Arakawa S, Harada H, Hausch G. Hilziuger H R, Menges F J, Warlimont H. In: Steeb S ed, Rapidly Quenched Metals, Vol. Ⅱ, Proc 5th Int Conf on Rapidly Quenched Metals, at Germany Sept., 3--7, 1984. North-Holland, 1985: 1389
8 Pang Dexing (庞德兴), Wang Jingtang (王景唐), Song Qihong (宋启洪), et al. J Phys D: Appl Phys, 1987; 20: 1544
9 Wang Jingtang (王景唐), Ding Bingzhe (丁炳哲), Li Shuling (李淑苓), Wei Xueli (隗学礼). In: Steeb S ed, Rapidly Quenched Metals, Vol. Ⅱ, Proc 5th Int Conf on Rapidly Quenched Metals, at Germany Sept., 3--7, 1984, North--Holland, 1985: 1361
10 Toeroek E. Hausch G, J Magn Magn Mater, 1979; 10: 303
No related articles found!
No Suggested Reading articles found!