A NEW KOSSEL ORIENTATION METHOD OF CRYSTAL
HUANG Rong;WANG Guanying Shanghai Institute of Metallurgy; Academia Sinica Manuscript received 18 October; 1987; revised manuscript 21 December; 1987
Cite this article: 

HUANG Rong;WANG Guanying Shanghai Institute of Metallurgy; Academia Sinica Manuscript received 18 October; 1987; revised manuscript 21 December; 1987. A NEW KOSSEL ORIENTATION METHOD OF CRYSTAL. Acta Metall Sin, 1988, 24(6): 514-517.

Download:  PDF(528KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new Kossel orientation method of crystal is developed. The distances among threeintersections of the Kossel lines on the indexed Kossel pattern observed are only necessary oforientation. Thus, the crror may be eliminated and the orientation preoision may be improved to±0.3°.
Key words:  Kossel orientation method     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/514

1 Yokowitz H. In: Tousimiss A J, Marton L eds., Advances in Electron Physics, Supplement 6, New York: Academic Press, 1969: 361
2 Peters E T, Ogilvie R E. Trans AIME. 1965; 233: 89
3 Rowlands P, Pevis M. Phys Status Solidi, 1968; 26: K25
4 Bevis M, Swindells N, Phys Status Solidi, 1967; 20: 197
5 Morris W G. J Appl Phys, 1968; 39: 1813
6 Halburg R, Ryder P L, Pitsch W. In: Proc 5th Int Conf on X-ray Optics and Microanalysis, Perlin: Springer-Verlag, 1969: 338
7 黄荣,张伟,王冠英.电子显微学报,1985;4:19
No related articles found!
No Suggested Reading articles found!