DYNAMIC SEGREGATION OF SULPHUR IN CAST IRON
QIN Ziqiang;YU Zongsen Beijing University of Iron and Steel Technology
Cite this article: 

QIN Ziqiang;YU Zongsen Beijing University of Iron and Steel Technology. DYNAMIC SEGREGATION OF SULPHUR IN CAST IRON. Acta Metall Sin, 1988, 24(6): 511-513.

Download:  PDF(814KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The segregation of sulphur at iron/graphite interfaces in both grey and nodular ironwas investigated with AES. Sulphur was found to nonequilibratorily segregated at the interfaces ingrey iron, but not in nodular iron. Such different behaviors of segregation, which will exaggeratethe difference of grey and nodular iron in sulphur content at ircn/graphite interfaces, might bederived from the difference of solidification process between the two irons.
Key words:  nodular iron      grey iron      sulphur distribution      dgnamic segregation     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/511

1 McSwain R H, Bates C E, Scott W D. Trans Am Foundrymen's Soc, 1974; 82: 85
2 Davis L E, MacDonald N C, Palmberg P W, Riach G E, Weber R E. Handbook of Auger Electron Spectroscopy, Edina: Physical Electronics Industries, 1972
3 McLean D. Grain Boundaries in Metals, Oxford: Clarendon Press, 1957: 121
4 Ohira G, Sato T, T, Sayama Y. In: Lux B et al. eds. The Metallurgy of Cast Iron, Proceedings of the Symposium, Switxerland, Geneva, May, 1974, Switzerland: Georgi Publishing Co. 1975: 295I
No related articles found!
No Suggested Reading articles found!