Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (4): 242-247    DOI:
Current Issue | Archive | Adv Search |
INVESTIGATION ON LATER STAGE OF INTERMEDIATE TRANSFORMATION IN Fe-C-Mo ALLOYS
XU Qikun;WANG Dongya Chongqing University Department of Metallurgy and Materials Engineering;Chongqing University; Sichuan
Cite this article: 

XU Qikun;WANG Dongya Chongqing University Department of Metallurgy and Materials Engineering;Chongqing University; Sichuan. INVESTIGATION ON LATER STAGE OF INTERMEDIATE TRANSFORMATION IN Fe-C-Mo ALLOYS. Acta Metall Sin, 1988, 24(4): 242-247.

Download:  PDF(1874KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The transformation process and the products of long term isothermaltransformation around the kinetic Bs temperature (the bay on TTT diagram) in Fe-C-Mo alloys have been investigated. It was found that, at the final stage of inter-mediate transformation, a sort of granular structure might form accompanying withthe growth of bainitic ferrite. In comparision with the carbide Mo_2C in the bainiticferrite plates and blockes, the carbide in granular eutectoid has been determined tobe (Fe, Mo)_3C type.
Key words:  Fe-C-Mo Alloy      intermediate transformation      kenetics     
Received:  18 April 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I4/242

1 Davenport E S, Bain E C, Kearny N J. Trans AIME. 1930; 90: 1117
2 徐启昆,何幼凡.金属热处理学报,1986;7(2) :91
3 徐启昆.重庆大学学报,1986;(3) :98
4 徐启昆,王东亚.材料科学进展,贝氏体相变专辑,1988;1(3) :41
5 A Letter from Reynolds W T Jr. 1986
6 Christian J W. The Theory of Transformations in Metals and Alloys, Part 1, Pergamon Press, 1981: 542
7 Kennon N F. Metall Trans, 1978; 9A: 57
8 Shiflet G J, Aaronson H I, The Incomplete Transformation (Stesis) Phenomenon in Fe-C-Mo Alloys, An unpublished Research in Carnegie-Mellon University, PA. 1982
9 Berry F G. Davenport A T, Honeycombe R W K. The Mech of Phase Tran sf in Crystalline Solids, London: The Inst of Metals, 1969: 288
10 Berry F G, Honeycombe R W K. Metall Trans, 1970; 1: 3279
11 Xu Qikun (徐启昆), Wang Jun (王俊), Wang Dongya (王东亚). Proc 11th Int Cong on Electron Microscopy, Kyoto: JSEM, 1986: 1267
[1] LUO Le;HU Suhui Shanghai Institute of Metallurgy; Academia Sinica. INFLUENCE OF GEOMETRICAL CONFIGURATION OF SUPERCONDUCTING MATERIAL ON GROWTH OF Nb_3Sn[J]. 金属学报, 1988, 24(5): 412-419.