Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (1): 104-110    DOI:
Current Issue | Archive | Adv Search |
AUGER-ION SPUTTERING ANALYSIS OF BINARY ALLOYS
QU Zhe;XIE Tiansheng Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

QU Zhe;XIE Tiansheng Institute of Metal Research; Academia Sinica; Shenyang. AUGER-ION SPUTTERING ANALYSIS OF BINARY ALLOYS. Acta Metall Sin, 1988, 24(1): 104-110.

Download:  PDF(627KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The element distribution of the homogeneous binary samples withmechanicaly scraped surfaces have been studied by means of Auger-Ion sputteringtechnique. The resulted profiling curves, generally show that the steady state con-centration usualy deviates more or less from the bulk concentration and that anobservable "spike" appears in the near surface layer. The amplitude of the divia-tion or the "spike" depends on the system and sputtering condition. Therefore, theAuger-Ion sputtering profiling curve could not reflect the original element distribu-tion exactly due to the interaction between energetic ions and atoms on the samplesurface. Some effects leading to the "distortion" and some aspects which must betaken in to account in using the profiling curve have been discussed briefly.
Key words:  Auger-Ion sputtering      scraped surfaces     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/104

1 Farber W. Betr G, Braun P. Nucl Instrum Methods, 1976; 132: 351
2 曲哲,孙玉珍,屠礼勋.分析化学,1986; 14: 753
3 Qu Zhe. Surf Sci, 1985; 161: L549
4 Kelly R. Surf Interface Anal, 1985; 7: 1
No related articles found!