ABRASIVE WEAR RESISTANCE OF Cr-FAMILY WHITE CAST IRONS |
by FANG Liang; RAO Qichang; ZHOU Qingde (Department of Mechanical Engineering; Xi'an Jiaotong University) (Manuscript received 11 August; 1985; revised manuscript 26 April; 1986) |
|
Cite this article:
by FANG Liang; RAO Qichang; ZHOU Qingde (Department of Mechanical Engineering; Xi'an Jiaotong University) (Manuscript received 11 August; 1985; revised manuscript 26 April; 1986). ABRASIVE WEAR RESISTANCE OF Cr-FAMILY WHITE CAST IRONS. Acta Metall Sin, 1987, 23(6): 575-580.
|
Abstract Abrasive wear resistance and fracturetoughness of white cast irons containing 2, 9, 15, 20 and 27 wt-%Cr have been investigated. Different contents of Cr and C have been added to the irons to keep the eutectic carbide constant (20—25%). Martensitic and austenitic matrices have been obtained by means of heat treatment. The results show that M_3C will transform to M_7C_3 and the microhardness of M_7C_3 itself will increase while the Cr/C ratio in iron increases. Meanwhile, the morph01ogy of carbides changes from Continuous network to rod or plate-like. All these make the carbides protect the matrices effectively, and improve the abrasive wear resistance of materials in pin-disc and wet rubber wheel wear tests. Wear resistance and fracture toughness have been discussed combinedly, that gives a general guide for designing and choosing wear resistant materials.
|
Received: 18 June 1987
|
1 Watson J D, Mutton P J, Sarse I R. Met Forum, 1980; 3(1) : 74-88 2 Gundlach R. B. Wear, 1978; 46: 97-108 3 Borik F. Met Eng Q, 1972; 12(2) : 33-39 4 Zum Gahr K-H, Eldis G T. Wear, 1980; 64: 175-194 5 Zum Gahr K-H. Metall Trans, 1980; 114(4) : 613-620 6 Maratray F. Factors Affecting the Structure of Chromium and Chromium-Moly-bdenum White Irons, Paris: Climax Molybdenum S A, 1971 7 Richardson R C D. Wear, 1968; 11(4) : 245-275 8 Xing J T, Lu W H, Wang X T. Wear of Materials, Int Conf on Wear of Materials, New York: ASME, 1983: 45-6 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|