THE INVESTIGATION OF EQUILIBRIUM BETWEEN SLAG AND HOT METAL CONTAINING Nb AND MEASUREMENT OF αNb_2O_5 IN THE SLAG
by CHEN Weiqing; ZHOU Rongzhang; LIN Zongcai (Beijing University of Iron and Steel Technology) (Manuscript received 6 June; 1986; revised manuscript 6 October; 1986)
Cite this article: 

by CHEN Weiqing; ZHOU Rongzhang; LIN Zongcai (Beijing University of Iron and Steel Technology) (Manuscript received 6 June; 1986; revised manuscript 6 October; 1986). THE INVESTIGATION OF EQUILIBRIUM BETWEEN SLAG AND HOT METAL CONTAINING Nb AND MEASUREMENT OF αNb_2O_5 IN THE SLAG. Acta Metall Sin, 1987, 23(6): 560-567.

Download:  PDF(570KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The reaction equilibrium between slag-hot metal containing Nb at temperature of hot metal pretreatment was investigated. Hot metal and slag containing Nb_2O_5 from Baotou was used. Meanwhile, a_([O] in molten iron was measured by means of the elctrolyte oxygen cell technique for calculating a_(Nb_2O_5) in slag. It was shown that when [Si]>0.02% and SiO_2/MnO<2,at the equilibrium state between slag-hot metal the selective removal of [Si] over [Nb] from Baotou hot metal is quite possible. The range of γ_(Nb_2O_5) values is 10°—10~(-2) at 1350℃. SiO_2/MnO of slag effects considerably on distribution ratio of Nb between slag-hot metal and on γ_(Nb_2O_5).

Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/560

1 福沢章.钢铁,1984;19(8) :56 2 陈伟庆,周荣章,林宗彩.钢铁,1987;22(5) :7 3 Schmalzried H. Ber Bunsenges Phys Chem, 1962; 66: 572 4 Elliott J F. Thermochemistry for Steeimaking, Vol. Ⅱ, Mass: Addison-Wesley, 1963 5 Janke D, Fischer W A. Arch Eisenhuettenwes, 1975; 46: 755 6 郭上型,唐仲和,张永定.全国第五届冶金物化年会论文集(上册),1984:157 7 罗晨,苏良赫.包钢含铌炼钢渣工业岩石学研究,武汉地质学院北京研究生部研究生论文,1983 8 Sigworth G K, Elliott J F. Met Sci, 1974; 8: 298 9 魏寿昆,张圣弼,佟亭,谭赞麟,钢铁.1984;19(7) :1 10 Schenck H, Steinmetz E. Wirkungsparameter Von Beglcitelementen flussiger Eisenloesungen und ihre gegenseitigen Beziehungen, Duesseldorf: Stahleisen-Sonderberichte, 1968: 39 11 日本铁钢学会.铁钢便霓,Ⅰ基礎,表1,3,第3版,东京:丸善,1981:22 12 张圣弼,佟亭,王济舫,魏寿昆.金属学报,1984;20:A 348 13 董元篪,彭(忄育)强,李丽芬,朱元凯,魏寿昆.全国第五届冶金物化年会论文集(上册),1984:217