HYDROGEN STORAGE PROPERTIES OF TiMnx ALLOYS
by QIAN Jiuxin; CHEN Jian; YE Yupu (Department of Chemistry; Peking University) (Manuscript received 10 May; 1986: revised manuscript 8 September; 1986)
Cite this article: 

by QIAN Jiuxin; CHEN Jian; YE Yupu (Department of Chemistry; Peking University) (Manuscript received 10 May; 1986: revised manuscript 8 September; 1986). HYDROGEN STORAGE PROPERTIES OF TiMnx ALLOYS. Acta Metall Sin, 1987, 23(6): 534-536.

Download:  PDF(227KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of alloy constituent, annealing heat treatment and reaction temperature on the hydrogen absorption and desorption properties for TiMn_x alloys has been investigated. The results show that the alloys containing 39—44 at. -%Ti exhibite excellent hydrogen desorption properties. They have MgZn_2 type Laves phase structure with a unit cell dimension of a=0.483—0.485nm and c=0.792—0.796nm. The hydrogen absorption capacity is 165 ml/g and the hydrogen desorption amount is 140ml/g for TiMn_(1.49)H system at 30℃.
Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/534

1 Gamo T, Moriwaki Y, Yanagihara N, Yamashita T, Iwaki T. In: Proc 3rd World Hyarogen Energy Conf, Vol. 4, Pergamon Oxford, 1980: 2127
2 Gamo T, Moriwaki Y, Yanagihara N, Iwaki T. J Less-Common Met, 1983; 89: 495
3 山下敏夫,蒲生孝治,森脇良夫,福田雅太郎,日本金属学会誌.1977;41:14
4 钱久信,毛英,叶于浦.金属学报,1987;23:A42
No related articles found!
No Suggested Reading articles found!