INITIATION AND GROWTH OF SURFACE CRACK UNDER TENSILE FATIGUE LOADING
by CHEN Siyi; LU Zhixian; ZHANG Dacheng; CUI Zhenyuan; (Northwestern Polytechnical University; Xi'an) (Manuscript reeieved 21 January; 1986; revised; manuscript 14 January; 1987)
Cite this article: 

by CHEN Siyi; LU Zhixian; ZHANG Dacheng; CUI Zhenyuan; (Northwestern Polytechnical University; Xi'an) (Manuscript reeieved 21 January; 1986; revised; manuscript 14 January; 1987). INITIATION AND GROWTH OF SURFACE CRACK UNDER TENSILE FATIGUE LOADING. Acta Metall Sin, 1987, 23(6): 514-520.

Download:  PDF(533KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of fatigue crack initial life, N., on the shape of initial notch and stress ratio under the tensile loading for LY12R sheet specimens has been studied. A relation predicting fatigue life, in N_i=a+b△K_c has been obtained. The crack growth behavior for LY12R, three steels and a titanium alloy have also been analysed. The results show that the crack growth behavior is not sensitive for materials, dimension of specimens and loading condition so that the surface crack depth may be predicted by the empirical expresion, △a=f(△c). It was also found that the surface crack extension is controlled by. stress strength. factor when σ_(Nmax)/σ_y=0.9.
Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/514

1 褚武扬,肖纪美,林实.力学学报,1979;(3) :294-297
2 陈思懿,卢智先,崔振源.力学与实践,1987;(3) :34-39
3 Newman J C Jr., Raju I S. Trans ASME J Pressure Vessel Technol, 1980; 102: 342
4 川原正言,栗原正好。日本造船学会论文集,1975;137:297-306
5 Nagai A, Toyosada M, Okamoto T. Eng Fract Mech, 1975; 7: 481-490
6 Truchon M. Lieurade H-P.5th Int Conf on Fracture, Cannes, France, 1981, Vol. 1, 33-39,
7 Cruse T. ASTM STP631, 1977: 179-189
No related articles found!
No Suggested Reading articles found!