Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (6): 470-476    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF MARTENSITE MORPHOLOGY AND CRYSTAL STRUCTURE ON THE PSEUDOELASTICITY IN A Cu-Al-Zn-Mn-Ni ALLOY
by YANG Jianhua; LIU Caihong; ZHAO Liancheng; LEI Tingquan (Harbin Institute of Technology) (Manuscript received 25 october; 1985; revised manuscript 15 July; 1986)
Cite this article: 

by YANG Jianhua; LIU Caihong; ZHAO Liancheng; LEI Tingquan (Harbin Institute of Technology) (Manuscript received 25 october; 1985; revised manuscript 15 July; 1986). INFLUENCE OF MARTENSITE MORPHOLOGY AND CRYSTAL STRUCTURE ON THE PSEUDOELASTICITY IN A Cu-Al-Zn-Mn-Ni ALLOY. Acta Metall Sin, 1987, 23(6): 470-476.

Download:  PDF(1124KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The deformation behaviour of parent phase and the pseudo-elasticity were studied, and the variation of microstructure with aging and deforming was analyzed using optical microscopy and X-ray diffraction. The experimental results showed that the pseudoelasticity in parent phase state is closely related to the original martensite microstructures. The pscudoelasticity of the alloy can be considerably improved with the perfection of martensitic self-accommodation and proper ageing treatment.
Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/470

1 Abu-Arab A, Chandrasekaran M, Ahlers M. Scr Metall, 1984; 18: 709
2 赵连城,杨建华,刘乃华,雷廷权.稀有金属,1986,5:281
3 Yang J H, Zhao L C, Zhang C S, Lei T C. Scr Metall, 1987; 21(3)
4 赵连城,杨建华,刘乃华,张春生,雷廷权,顾华,何永枢.金属学报,1987;23A380:
5 Delaey L, Krishnan R V, Tas H, Warlimont H. J Mater Sci, 1974; 9: 1521
6 Van Humbeeck J. Janssen J, Mwamba-Ngoie, Delaey L. Scr Metall, 1984; 18: 893
7 Delaey L, Suzuki T, Van Humbeeck J. Scr Metall, 1984; 18: 899
No related articles found!
No Suggested Reading articles found!