Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (6): 464-469    DOI:
Current Issue | Archive | Adv Search |
HIGH VOLTAGE TEM OBSERVATION OF THERMOELASTIC MARTENSITIC TRANSFORMATION IN A Cu-Zn-Al ALLOY
by DENG Yongrui (Beijing University of Iron and Steel Technology); ANSELL; G. S.. (Rensselaer Polytechnic Institute; USA) (Manuscript received 3 December; 1985; revised manuscript 28 May; 1985)
Cite this article: 

by DENG Yongrui (Beijing University of Iron and Steel Technology); ANSELL; G. S.. (Rensselaer Polytechnic Institute; USA) (Manuscript received 3 December; 1985; revised manuscript 28 May; 1985). HIGH VOLTAGE TEM OBSERVATION OF THERMOELASTIC MARTENSITIC TRANSFORMATION IN A Cu-Zn-Al ALLOY. Acta Metall Sin, 1987, 23(6): 464-469.

Download:  PDF(3216KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The martensitic transformation in Cu-29%Zn-3%Al alloy occurs thermoelastically. High voltage TEM observation shows that the parent phase belongs to DO_3 and martensite belongs to 18R in structure. Fine structures of tiny packages with a traverse size of~10nm in martensite plates have been seen at the thicker part of the sample. The boundary between β' and M at the thinner part was flat or sawtooth-like composed parallel dislocation lines: Although the reversibility of the transformation in TEM samples has been observed under an optical microscope, only the β'→M transformation observed on TEM. Probably, the thickness of thiner part of the foil is too small to store enough elastic energy which is the driving force of the reverse transformation.
Received:  18 June 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I6/464

1 武沢和羲,佐藤博保,阿部良贤,佐藤进一.日本金属学会志,1979;43:235
2 Balcelo G, Rapacioli R, Ahlers M. Scr Metall, 1978; 12: 1069
3 Takezawa K, Izumi T, Chiba H, Sato S. In: ICOMAT-82, Lelaey L ed., International Conference on Martensitic Transformations, at Leuven August 1982, Belgium, 1982: 813
4 Chakravorty S, Wayman CM. Acta Metall, 1977; 25: 989
5 Tadaki T, Katsuki K, Shimizu K. Symposium on New Aspects of Martensitic Transformations, JIM, Kobe, Japan. 1976: 187
6 Lovey F C. In: ICOMAT-82, Lelaey L ed., International. Conference on Martensitic Transformations. at Leuven August 1982, Belgium, 1982: 585
7 Deng Y. Doctoral Thesis, 1984, Rensselaer Polytechnic Institute, USA
No related articles found!
No Suggested Reading articles found!