Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (5): 468-473    DOI:
Current Issue | Archive | Adv Search |
PLASTICITY AND TRIAXIALITY IN STRUCTURAL STEEL AND ASSOCIATED WELD METALS
by SHI Yaowu; ZHU Denghe; SUN Yuping (Xi'an Jiaotong University)(Manuscript received 15 January; 1985; revised manuscript 11 November; 1985)
Cite this article: 

by SHI Yaowu; ZHU Denghe; SUN Yuping (Xi'an Jiaotong University)(Manuscript received 15 January; 1985; revised manuscript 11 November; 1985). PLASTICITY AND TRIAXIALITY IN STRUCTURAL STEEL AND ASSOCIATED WELD METALS. Acta Metall Sin, 1987, 23(5): 468-473.

Download:  PDF(733KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In order to assess the effect of stress triaxiality on the plasticity and ductility of the structural mild steel and the associated weld metals, the tensile tests on notched round bar specimens were performed. The results indicated that the strains to initiate failure for the boiler steel and weld metals were a strong function of stress states. Under the same triaxiality the failure initiation strain of J427 weld metal was the largest among these materials, and that of J422 weld metal was the smallest. Moreover, the material constant C values relating to the metallurgical characteristics were given for the experimental steel and weld metals.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/468

1 Milne I, Curry D A. In: Radon J C ed., Fracture and Fatigue, Proc 3rd European Conf on Fracture, Oxford: Pergamon, 1980: 39
2 Hancock J W, Cowling M J. Met Sci, 1980; 14: 293
3 Shi Y W (史耀武), Barnby J T, Nadkarni A S. In: Valluri S R et al, eds., Advances in Fracture Research, Proc 6th Int Conf on Fracture, Oxford: Pergamon, 1984: 1329
4 Mackenzie A C, Moakler M. In: Pressure Vessel Technology, Part 2, ASME, 1973: 1167
5 Bridgman P W. Studies in Large Flow and Fracture, New York: McGraw-Hill, 1952
6 Rice J R, Tracey D W. J Mech Phys Solids, 1969; 17: 201
7 Shi Y W (史耀武), Barnby J T. Int J Fract, 1984; 25: 14
No related articles found!
No Suggested Reading articles found!