IN SITU OBSERVATION OF THE FRACTURE FOR A SPHEROIDIZED LOW CARBON STEEL
by ZHANG Yizeng; DAI Shujuan; ZOU Hongcheng; MIAO Pifeng (Huazhong University of Science and Technology; Wuhan)(Manuscript received 23 January; 1986; revised manuscript 23 July; 1985)
Cite this article: 

by ZHANG Yizeng; DAI Shujuan; ZOU Hongcheng; MIAO Pifeng (Huazhong University of Science and Technology; Wuhan)(Manuscript received 23 January; 1986; revised manuscript 23 July; 1985). IN SITU OBSERVATION OF THE FRACTURE FOR A SPHEROIDIZED LOW CARBON STEEL. Acta Metall Sin, 1987, 23(5): 403-407.

Download:  PDF(1991KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In situ observations of the behavior of void formation and dislocations formed ahead of a crack in a spheroidized low carbon steel have been carried out during fracture tests with TEM. The results show that the fracture occurs through alternate processes of nucleation, growth and coalescence of voids during plastic deformation. Void coalescence generally associates with the necking of matrix metal between the voids. Most frequetly, the cracks are in a zigzag shape. The deformation on the two sides of a zigzag crack does not match microscopically with each other. Dislocations may emit from the crack tip when the crack is either propagating or blunting. The dislocation emission is the main cause of the crack blunting. The effect of dislocation distribution on the void formation has also been discussed.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/403

1 Wilsdorf H G F. ASTM STP 245, 1958: 43
2 Forsyth P J E, Wilson RN. J Inst Met, 1963; 92: 82
3 Kuhlmann-Wilsdorf D, Wilsdorf H G F. JAppl Phys, 1960; 31: 516
4 Kobayashi S, Ohr SM. Philos Mag, 1980; A42: 763
5 Ohr SM, Narayan J. Philos Mag, 1980; A41: 81
6 Chang C-J, Ohr SM. JAppl Phys, 1981; 52: 7174
7 Ashby MF. Philos Mag, 1966; 14: 1157
8 张以增,金属学报,1983;19:A70
9 ZOU H-C(邹鸿承),Lou Y-L(娄彦良),Zhang Y-Z(张以增).Mater Sci Eng,1984;62:163
No related articles found!
No Suggested Reading articles found!