Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (5): 396-402    DOI:
Current Issue | Archive | Adv Search |
CORROSION FATIGUE CRACK INITIATION IN A MODE Ⅱ NOTCH SPECIMEN
by CHU Wuyang; XIAO Jimei (C. M. Hsiao); ZHAO Yusheng (Beijing University of Iron and Steel Technology)(Manuscript received 27 August; 1985)
Cite this article: 

by CHU Wuyang; XIAO Jimei (C. M. Hsiao); ZHAO Yusheng (Beijing University of Iron and Steel Technology)(Manuscript received 27 August; 1985). CORROSION FATIGUE CRACK INITIATION IN A MODE Ⅱ NOTCH SPECIMEN. Acta Metall Sin, 1987, 23(5): 396-402.

Download:  PDF(1540KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The stress intensity K_Ⅱ of a mode Ⅱ specimen was calculated using a finite element method via the J integral. The site direction and threshold value for crack initiation from the notch under cyclic mode Ⅱ loading in air, in water and under dynamic charging with hydrogen were investigated. The results showed that the mode Ⅱ fatigue crack in a high strength steel initiated at or close to the site of the maximum principal stress, rather than at the site of the maximum shear stress, and the subsequent crack growth was orientated approximately normal to the direction of the maximum principal stress. The site and direction of crack initiation in water and under dynamic charging with hydrogen were similar but different from that in air. The threshold values for crack initiation in air, in water and under dynamic charging were 28.8, 12.3 and 10.2 MPa·m~(1/2), respectively. The fracture surface of a corrosion fatigue crack in water and under dynamic charging consisted of intergranular facets at low △K_Ⅱ values but of quasi-cleavage at higher △K_Ⅱ values and were different than those in air.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/396

1 Kocanda S. Fatigue Failure of Metals, Warsaw: Sijthoff and Noordhoff international publishers, 1978
2 Chu W Y (褚武扬), Hsiao C M. (肖纪美), Liu TH (刘天化). Fatigue Eng Mater Struct 1984; 7: 279
3 张统一,褚武扬,肖纪美,李英,金属学报,1986;22:A349.
4 中国航空研究院主编.应力强度因子手册,科学出版社,1981;122
5 Wang YB(王燕斌),chu WY(褚武扬),Hsiao CM(肖纪美).Scr Metall,1985;19:1161
6 张统一,褚武扬,肖纪美.中国科学,A,1986;(3) :316#
No related articles found!