EFFECT OF Cr ON P GRAIN BOUNDARY SEGREGATION IN LOW ALLOYED STEELS
by ZHAO Yuxin;LI Pengxing; XU Zuyao (T. Y. Hsu)(Shanghai Jiaotong University)(Manuscript received 4 February; 1985)
Cite this article: 

by ZHAO Yuxin;LI Pengxing; XU Zuyao (T. Y. Hsu)(Shanghai Jiaotong University)(Manuscript received 4 February; 1985). EFFECT OF Cr ON P GRAIN BOUNDARY SEGREGATION IN LOW ALLOYED STEELS. Acta Metall Sin, 1987, 23(5): 356-361.

Download:  PDF(517KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Since carbon is a more intensive grain boundary active element and would replace the impurity at the grain boundary of steels, the grain boundary segregation of the impurity would be controlled by the carbon solubility in a-phase. The alloying elements, decreasing - the carbon solubility, would enhance the impurity segregation at the grain boundary. With this point of view, a new modified Guttmann's model is suggested from which the calculated results are in good agreement with the experimental data in carbon and Cr steels.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/356

1 Krahe P R, Guttmann M. Scr Metall, 1973; 7: 387
2 Joshi A, Stein D F. ASTM, STP 499, 1972: 59
3 Mulford RA, McMahon C J Jr, Pope D P, Feng H C. Metall Trans, 1976; 7A: 1183
4 Low J R, Stein D F, Turkalo A M, Laforce R P. Trans AIME, 1968; 242: 14
5 Guttmann M. Surf Sci, 1975; 53: 213
6 Guttmann M, McLean D. In: Johson WC, Blakely J M eds., Interfacial Segregation, Ohio: ASM, 1979: 251
7 Guttmann M, Dumoulin Ph, Wayman M. Metall Trans, 1982; 13A: 1693
8 Erhart H, Grabke HJ. Metall Sci, 1981; 15: 401
9 Uhrenius B. In: Doane D V, Kirkaldy JS eds., Hardenability Concepts with Application to Steels, New York: AIME, 1978: 28
10 Yu J, McMahon CJ, Jr. Metall Trans, 1980; 11A: 277, 291
11 Qu Z, Kou KH. Metall Trans, 1981; 12A: 1333
12 Dumoulin Ph, Guttmann M. Mater Sci Eng, 1980; 42: 249
13 Maurer M, Cadeville M C, Sanchez J P.Philos Mag, 1978; A38: 739
14 Wada T, Wada H, Elliott J F, Chipman J. Metall Trans, 1971; 2A: 2199
15 Kirchner G, Nishizawa T, Uhrenius B. Metall Trans, 1973; 4A: 167
16 Wada T, Wada H, Elliott J F, Chipman J. Metall Trans, 1972; 3A: 1657
No related articles found!
No Suggested Reading articles found!