| EFFECT OF DISLOCATION IMAGE FORCE ON DISLOCATION DISTRIBUTION IN PLASTIC ZONE AT CRACK TIP |
| by LIU Su; XIONG Liangyue; LONG Qiwei(C. W. Lung)(Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 17 July; 1985; revised manuscript 17 April; 1986) |
|
Cite this article:
by LIU Su; XIONG Liangyue; LONG Qiwei(C. W. Lung)(Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 17 July; 1985; revised manuscript 17 April; 1986). EFFECT OF DISLOCATION IMAGE FORCE ON DISLOCATION DISTRIBUTION IN PLASTIC ZONE AT CRACK TIP. Acta Metall Sin, 1987, 23(5): 349-355.
|
|
|
Abstract The equilibrium dislocation distribution in the plastic zone at a crack tip has been calculated, where the influence of image force of dislocation was involved. The results were compared with that in which dislocation image force was omitted. A maximum value α_c was obtained for the applied stress level α, and thus a critical value α_c was correspondingly obtained for the size of plastic zone α, The dislocation image force makes the plastic zone become large while α<α_c, and the ligament yielding takes place if α>α_c. This qualitatively agrees with the experimental results of positron annihilation measurement published be fore.
|
|
Received: 18 May 1987
|
1 龙期威,熊良钺.物理学报,1984;33:755 2 Bilby B A, Cottrell A H, Swinden K H. Proc R Soc London, 1963; A272: 304 3 Kobayashi S, Ohr SM. Philos Mag, 1980; A42: 763 4 Chang SJ, Ohr SM. JAppl Phys, 1981; 52: 7174 5 Lung CW, Xiong L Y. Phys Status Solidi, (a), 1983; 77: 81 6 Jiang J, Xiong L Y, Lung C W, Ji G K, Liu N Q, Wang S Y. In: Coleman P G et al eds., Proc 6th Int Conf Positron Annihilation, held at Arlington, New York: North-Holland, 1982: 469= |