| CORRELATION BETWEEN STACKING FAULT ENERGY AND CREEP PROPERTY OF SOLID SOLUTION STRENGTHENING SUPERALLOYS |
| by MENG Qing'en; XI Xiurong (Central Institute of Iron and Steel Research; Ministry of Metallurgy Industry; Beijing) (Manuscript received 18 December; 1985; revised manuscript 18 April; 1986) |
|
Cite this article:
by MENG Qing'en; XI Xiurong (Central Institute of Iron and Steel Research; Ministry of Metallurgy Industry; Beijing) (Manuscript received 18 December; 1985; revised manuscript 18 April; 1986). CORRELATION BETWEEN STACKING FAULT ENERGY AND CREEP PROPERTY OF SOLID SOLUTION STRENGTHENING SUPERALLOYS. Acta Metall Sin, 1987, 23(4): 344-345.
|
|
|
Abstract Determination of the stacking fault energy, Y, of the solid solution strengthening superalloys with various contents of Co and W with relation to their steady-state creep rate, s was carried out by X-ray texture method. The stacking fault energy decreases with the increase of Co and W. An expression may be proposed as ε ∞ γ~m, where m=1.46.
|
|
Received: 18 April 1987
|
1 Dillamore I L, Smallman R E, Roberts W T. Philos Mag, 1964; 9:517 2 Smallman R E, Green D. Acta Metall, 1964; 12(2) : 145 3 Davies C K L, Davies P W, Wilshire B Philos Mag, 1965; 12: 827 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|