ON THE CALCULATION OF DRIVING FORCE FOR MARTENSITE TRANSFORMATION AND M_s IN Fe-Ni-C ALLOYS
by LI Jian; XU Zuyao (T.Y. Hsu) (Shanghai Jiaotong University) (Manuscript received 17 February; 1985)
Cite this article: 

by LI Jian; XU Zuyao (T.Y. Hsu) (Shanghai Jiaotong University) (Manuscript received 17 February; 1985). ON THE CALCULATION OF DRIVING FORCE FOR MARTENSITE TRANSFORMATION AND M_s IN Fe-Ni-C ALLOYS. Acta Metall Sin, 1987, 23(4): 321-328.

Download:  PDF(570KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The driving force for martensite transformation,-△G_(M_S)~(γ→α)(=△G~(α→M)) has been evaluated using three different thermodynamic methods, namely, LFG method, Hsu method and the authors' method. The results show that the relationship between driving force and σ_(0.2)(M_s) can be expressed as: AG~(α→M)=A'σ(M_s)+908 J/mol wher eA' is a constant which slightly deviated for different methods. The M_s temperatures of Fe-Ni-C alloys have been calculated, and the results of calculation are in good agreement with the previous experimental values.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/321

1 Zener C. Trans AIME, 1946; 167:550
2 Fisher J C. Trans AIME, 1949; 185: 688
3 Rao M M, Russell R J, Winchell P G. Trans Metall Soc AIME, 1967; 239:634
4 Scheon F J, Owen W S. Metall Trans 1971; 2:2431
5 徐祖耀.金属学报,1980;16:420,426;J Mater.Sci,1985;20:23
6 徐祖耀,李箭,曾振鹏.金属学报,1986;22:A494
7 Bhadeshia H K D H. Met Sci, 1981; 15:178
8 徐祖耀,马氏体相变与马氏体,北京:科学出版社,1980:253
9 Hsu T Y(Xu Zuyao), Zhang Hongbing. Acta Metall, 1984; 32:343
10 Aaronson H I, Domian H A, Pound G M. Trans Metall Soc AIME, 1966; 236:753
11 Zener C. Trans AIME, 1955; 203:619
12 Mon Yiwen, Hs(?) T Y(Xu Zuyao). Acta Metall, 1986; 34: 325
13 Mogutnov B M, Tomilin I A, Shvarsman L A. Thermodynamic of Fe-C Alloys, Moscow: Metallurgy Press, 1972:10
14 张鸿冰,倪乐民,徐祖耀.金属学报,1987;23:A42
15 Kaufman L. In: Rudman P S, Stringer J, eds. Phase Stability in Metals and Alloys, New York: McGraw-Hill, 1967: 125
16 Breedis J F, Kaufman L. Metall Trans, 1971; 2:2359
17 Kaufman L, Clougherty E V, Weiss R J. Acta Metall, 1963; 11:323
18 Swartz J C. Trans Metall Soc AIME, 1969; 245:1083
19 Wada T, Wada H, Elliott J F, Chipman J. Metall Trans, 1971; 2:2199
20 Kaufman L, Radcliffe S V, Cohen M. In: Zackay V F, Aaronson H I, eds. Decomposition of Austanite by Diffusional Processes, New York:Interscience, 1962: 313
21 Orr R L, Chipman J. Trans Metall Soc AIME, 1967; 239:630
22 Bhadeshia H K D H. Met Sci, 1981; 15:175
23 Steven W, Haynes A G. J Iron Steel Inst, 1961; 197:199
24 Rao M M, Winchell P G. Trans Metall Soc AIME, 1967; 239:956
No related articles found!
No Suggested Reading articles found!