A COMPLEX DEFORMATION MECHANISM FOR SUPERPLASTIC DEFORMATION OF Mg ALLOY
by CHEN Puquan; ZHAO Min (Harbin Institute of Technology) (Manuscript received 10 May; 1985; revised manuscript 15 February; 1986)
Cite this article: 

by CHEN Puquan; ZHAO Min (Harbin Institute of Technology) (Manuscript received 10 May; 1985; revised manuscript 15 February; 1986). A COMPLEX DEFORMATION MECHANISM FOR SUPERPLASTIC DEFORMATION OF Mg ALLOY. Acta Metall Sin, 1987, 23(4): 313-320.

Download:  PDF(1404KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Study was made of the superplastic deformation mechanism for two selected Mg alloys of either coarse or superfine grain by means of an advanced testing technique. It was shown that the mechanism under superplastic deformation for these two alloys is mainly due to the grain boundary sliding together with the coordination of diffusion creep and dislocation slip. A complex deformation mechanism model including the above mentioned three ones is believed to be proposed. The metal grains may progressively emerge from underneath up to surface during superplastic deformation through grain boundary sliding in the site on which the broadening and cavities along transverse grain boundaries appeared, thus, the number of grains along the tensile axis may be continuously incressed. This seems to be the origin of the extreme elongation of the specimen under tensile deformation.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/313

1 Ashby M F, Verall R A, Acta Metall, 1973; 21: 149
2 Novikov I I. Acta Metall, 1977; 10: 1139
3 Ball A, Hutchison M M. Met Sci J, 1969; 3: 1
4 Mukherjee A K. Mat Sci Eng, 1971; 8: 83
5 Spingarn J R, Nix W D. Acta Metall, 1979; 27: 171
6 Gifkins R C. Metall Trans. 1976; 17: 1225
7 Gifkins R C. J Mater Sci, 1978: 13: 1926
8 Geckinli A E. Met Sci, 1983; 17: 12
9 杨金风,陈浦泉.宇航学报,1984;1:44
10 陈浦泉,赵敏.金属热处理,1984;(9) :23
11 陈浦泉,赵敏.金属科学与工艺,1985;4(1) :33
12 Chen Puquan(陈浦泉), Zhao Min(赵敏). In: Pro 7th Int Conf on the Strength of Metals and Alloys, New York: Pergamon Press, 1985; 2: 817g
No related articles found!
No Suggested Reading articles found!