Acta Metall Sin  1987, Vol. 23 Issue (4): 253-261    DOI:
Current Issue | Archive | Adv Search |
A NEW VIEWPOINT ON MECHANISM OF PREFERENTIAL SPUTTERING OF Au-Cu ALLOYS
by LI Risheng (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 30 December; 1985; revised manuscript 15 June; 1986)
Cite this article: 

by LI Risheng (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 30 December; 1985; revised manuscript 15 June; 1986). A NEW VIEWPOINT ON MECHANISM OF PREFERENTIAL SPUTTERING OF Au-Cu ALLOYS. Acta Metall Sin, 1987, 23(4): 253-261.

Download:  PDF(806KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new viewpoint on the mechanism of preferential sputtering of Au-Cu alloys suggests that the so-called preferential sputtering in Au-Cu alloys may be caused by the bombardment-induced Gibbsian segregation, but when ion energy decreases to,ward a near-threshold condition, the maBs-correlating preferential sputtering also plays a role.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/253

1 Behrisch R. Sputtering by Particle Bombardment 1 and 2, Berlin: Springer, 1981 and 1983
2 Wehner G K. In: Czanderna A W ed. Methods of Surface Analysis, Amsterdan: Elservier, 1975: 5
3 Betz G. Surf Sci, 1980; 92; 283
4 Kelly R. Surf Sci, 1980; 100: 85
5 Li R S(李日升), Koshikawa T, Goto K.Surf Sci, 1982; 121: L 561
6 Patterson W L, Shirn G A. J Vac Sci Technol, 1967; 4: 343
7 Pickering H W. J Vac Sci Technol, 1976; 13: 618
8 Ho P S 何兆中. Surf Sci, 1978; 72: 253
9 Koshikawa T, Goto K, Saeki N Shimizu R, Sugata E. Surf Sci 1979; 79: 461
10 Okutani T, Shikata M, Shimizu R. Surf Sci, 1980; 99: L410 Kang H J,Shimizu R, Okutani T. Surf Sci, 1982; 116: L173
11 Swartzfager D G, Ziemecki S B, Kelley M J. J Vac Sci Technol, 1981; 19: 185
12 Farber W, Betz G, Braun P. Nucl Instrum Methods, 1976; 132: 351
13 Tompkins H G. J Vac Sci Technol, 1976; 16: 778
14 Ichimura S, Shimizu R, Ikuda T. In: Johari O, Scanning Electron Microscopy, AMF O'Hare,IL, 1981
15 LiR S (李日升),Koshikawa T, Goto K,In: Proc Ann Meeting Japan Society of Applied Physics, 1981: 254
16 Ho P S, Lewis J E, Wildman H S, Howard J K. Surf Sci, 1976; 57: 393
17 Kelly R. Surf Interface Anal, 1985; 7: 1
18 Kelly R.私人通讯,1984
19 Li R S (李日升), Koshikawa T. Surf Sci 1985; 151: 459
20 See, For example, Okamoto P R, Rehn L E. J Nucl Mater, 1979; 83: 2, and references therein
21 Li R S (李日升), Tu L X (屠礼勋), Sun Y Z (孙玉珍). Surf Sci, 1985; 163: 67.
22 LiRS (李日升), TuLX (屠礼勋), Sun Y Z(孙玉珍). Appl Surf Sci, 1986; 26: 77
23 Betz G, Braum P, Farber W. J Appl Phys, 1977; 48: 1404
24 Nakamura H, Morita K, Itoh N. Nucl Instrum Methods, 1981; 191: 119
25 Holloway P H, Bhattacharya R S. J Vac Sci Technol, 1982; 20: 444
26 Itoh N, Morita K. Radiat Eff, 1984; 80: 163
27 Andersen H H, Stenum B, Sorensen T, Whitlow H J. Nucl Instrum Methods, 1983; 209/210: 487
28 Sigmund P, Oliva A, Falcone G. Nucl Instrum Methods, 1982; 194: 541
No related articles found!