THERMAL STABILITY OF AMORPHOUS Fe-Co-Si-B THIN FILM PREPARED BY SPUTTERING
FENG Qun; FENG Minying; WANG Yizhong; WANG Zhenxi(Institute of Physics; Academia Sinica; Beijing) (Manuscript received 16 August; 1985; revised manuscript 6 May; 1986)
Cite this article: 

FENG Qun; FENG Minying; WANG Yizhong; WANG Zhenxi(Institute of Physics; Academia Sinica; Beijing) (Manuscript received 16 August; 1985; revised manuscript 6 May; 1986). THERMAL STABILITY OF AMORPHOUS Fe-Co-Si-B THIN FILM PREPARED BY SPUTTERING. Acta Metall Sin, 1987, 23(3): 288-290.

Download:  PDF(800KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The thermal stability of amorphous Fe_78Co_4.3Si_5.9B_11.8 thin film prepared by sputtering has been studied using thermomagnatie measurements, differential thermal analysis, electron microscopic analysis, electron diffraction and X-ray diffraction. It is observed that the crys-tallization process of sputtering film is different from that of melt quenching ribbons. The crystallization temperature of the former is much lower than that of latter. The preparing condition have an important effect on the thermal stability.
Received:  18 March 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I3/288

1 Egami T, Dahlgren S D, J Appl Phys, 1978; 49: 1703
2 Tsumashima S, Mitruya S, uchiyama S. Jpn J Appl Phys, 1981; 20: 727
3 Herold U, Koster U, Dirks A G. J Magn Magn Mater, 1980; 19: 15
No related articles found!