Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (3): 271-318    DOI:
Current Issue | Archive | Adv Search |
BAINITIC TRANSFORMATION IN NODULAR CAST IRON
SHI Deke; GUO Dazhan; SONO Xiaoping(Xi'an jiaotong University) (Manuscript received 9 Octorber; 1984; revised manuscript 10 January; 1986)
Cite this article: 

SHI Deke; GUO Dazhan; SONO Xiaoping(Xi'an jiaotong University) (Manuscript received 9 Octorber; 1984; revised manuscript 10 January; 1986). BAINITIC TRANSFORMATION IN NODULAR CAST IRON. Acta Metall Sin, 1987, 23(3): 271-318.

Download:  PDF(1456KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The temperature which separates upper and lower bainitic transformations is about 300℃ in nodular cast iron. The overall activation energy of lower bainitic transformation of it is nearly the same as that for high carbon steels, but that of upper bainitic transformation is much smallar than the value of latter. this can be explained by the fact that the addition of Si suppresses precipitation of Fe_3C. The following orientation relationships have been observed by the present work: N-W relation for ferrite and austenite in upper bainite; K-S relation for ferrite and austenite in lower bainite and Bagaryatski relation for Fe_3C and ferrite in lower bainite.
Received:  18 March 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I3/271

1 Johansson M. Trans Am Foundrymen's Soc, 1977; 85: 117
2 Janowak J F. Mod Cast, 1981; 71(12) : 34
3 石德珂,郭大展,柴惠芬.西安交通大学学报,1983;(2) :27
4 Cahn R W, Physical Metallurgy, 2nd ed., Amsterdam: North-Holland, 1970
5 Zener C. J Appl Phys, 1949; 20: 950
6 Bhadeshia H K D H, Edmond D C. Metall Trasns, 1979; 10 A: 895
7 Robert C S. Trans AIME, 1953; 197: 203
8 Radicliffe I V, Rollason E S. J Iron Steel Inst, 1958; 191: 56
9 White H S, Owen W S. J Iron Steel Inst. 1958; 195: 79
10 俞德刚,石德珂.第一届全国热处理年会论文集,机械工业出版社,1964:105)
No related articles found!