LOW CYCLE FATIGUE OF STEEL 35 UNDER TORSIONAL STRAIN
ZHAO Tingshi; LIU Dunkang; JI Huijun(Huazhong University of Science and Technology; Wuhan) (Manuscript received 31 December; 1984; revised manuscript 10 July; 1986)
Cite this article: 

ZHAO Tingshi; LIU Dunkang; JI Huijun(Huazhong University of Science and Technology; Wuhan) (Manuscript received 31 December; 1984; revised manuscript 10 July; 1986). LOW CYCLE FATIGUE OF STEEL 35 UNDER TORSIONAL STRAIN. Acta Metall Sin, 1987, 23(2): 156-157.

Download:  PDF(174KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Studies were made of the material performance of steel 35 under low cycle torsion as well as the relationship of the low cycle torsional fatigue life together with the torsional strain amplitude and fatigue energy under torsion strain. The feature of the fatigue failure of the steel under low cycle torsion was also discussed.
Received:  18 February 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I2/156

1 徐灏,疲劳强度设计.机械工业出版社,1981,277-288
2 Hertzberg R W.工程材料的变形与断裂力学,王克仁等译.1982,495
3 谢济洲.机械强度,1980;(11) :75-83
No related articles found!
No Suggested Reading articles found!