Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (2): 150-245    DOI:
Current Issue | Archive | Adv Search |
A DYNAMIC OBSERVATION OF MICROSCOPIC DEFORMATION BEHAVIOR IN DUAL-PHASE STEELS
SHEN Xianpu (Central Tron and Steel Research Institute; Ministry oj Metallurgical Industry; Beijing); LEI Tingquan; LIU Jianzhuang (Harbin Institute of Technology) (Manuscript received 21 May; 1985; revised manuscript 28 April; 1986)
Cite this article: 

SHEN Xianpu (Central Tron and Steel Research Institute; Ministry oj Metallurgical Industry; Beijing); LEI Tingquan; LIU Jianzhuang (Harbin Institute of Technology) (Manuscript received 21 May; 1985; revised manuscript 28 April; 1986). A DYNAMIC OBSERVATION OF MICROSCOPIC DEFORMATION BEHAVIOR IN DUAL-PHASE STEELS. Acta Metall Sin, 1987, 23(2): 150-245.

Download:  PDF(1674KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Microscopic deformation behavior in some dual-phase steels consisting of ferrite and martensite has been observed continuously by using a scanning electron microscope with tension stand, and the strain values of two phases have been measured with graphanalyse technique. The results show that the distribution of strain between two phase and that in each phase are so nonuniform as to cause a strain gradient in front of martensite islands. The ratio of strain in martensite to that in ferrite increases with the increase of martensite content and tempering temperature as well as the decrease of carbon content in marteniste. The yield strength of dual phase steel with ferrite matrix is controlled by the ferrite.
Received:  18 February 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I2/150

1 沈显璞,雷廷权.金属学报,1985;21:A228
2 沈显璞,雷廷权.金属学报,1984;20:A266
3 Shen H P (沈显璞),Lei T C(雷廷权).Met Sci 1984; 19: 275
4 田村今男,友田陽,山岡幸男,金谷三郎,小沢正俊,赤尾明,鉄鋼,1973;59:454
5 Davies R G. Metall Trans 1978; 9A: 451
6 Araki K, Takada Y, Nakaoka K. Trans Ionr Steel Inst Jpn 1977; 17:710
7 Tomota Y, Kuroki K, Mori t, Tamura I. Mater Sci Eng 1976; 24: 85
8 雷廷权,沈显璞,金属学报,1982;18:75
9 Lei TC(雷廷权),Shen HP(沈显璞). In: MC Queen H J, Bailon J-P, et al eds Strength of Metals and Alloys. New York: Oxford, Pergamon Press, 1985, Vol. 2: 1007
10 Davies R G. Metall Trans 1978; 9A: 691
11 Wan C M, Yie S N,Jahn M T,Kuo S M.J Meatr Sci 1981; 16: 2682
No related articles found!