THERMODYNAMICAL STUDY OF INTERACTION BETWEEN NITROGEN AND Ce OR Y IN LIQUID IRON
YUE Kexiang DU Ting LI jizong SHEN Rumei (Central Iron and Steel Research Institute;Ministry of Metallurgical Industry;Beijing)
Cite this article: 

YUE Kexiang DU Ting LI jizong SHEN Rumei (Central Iron and Steel Research Institute;Ministry of Metallurgical Industry;Beijing). THERMODYNAMICAL STUDY OF INTERACTION BETWEEN NITROGEN AND Ce OR Y IN LIQUID IRON. Acta Metall Sin, 1987, 23(1): 99-102.

Download:  PDF(249KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Equilibria of the Fe-Ce-N and Fe-Y-N melts with very low oxygen and sulphur conte- nts have been investigated at 1570—1650℃.The equilibriun products are examined to be CeN and YN respectively.The temperature dependences on their interaction coefficients are determined to be: e_N~(Ce)=-(6230/T)+2.670;e_(Ce)~N=-(62281/T)+26.64 e_N~Y=-(6640/T)+2.986;e_Y~N=-(41991/T)+18.83 That on denitriding constants are: 1g K_(CeN)~°=-(20960/T)+7.972;1g K_(YN)=-(20440/T)+7.863 That on standard free energy of formation of CeN and YN are: △G_(CeN)~°=-401204+152.59T(J/mol) △G_(YN)~°=-391246+150.50T(J/mol) That on self-interaction coefficients are: e_(Ce)~(Ce)=-(79.92/T)+0.0167;e_Y~Y=-(64.51/T)+0.0142
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/99

1 #12
2 Fisher,W.A.Berfram H.,Arch Eisenhuettenws.,1973;44:87
3 日本铁钢协会编.铁钢便览,第Ⅰ卷:基础.第三版,东京:丸善.1981;15.
No related articles found!
No Suggested Reading articles found!