Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (1): 50-56    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF SMALL ALLOYING ADDITIVES ON FORMATION OF Nb_3Sn LAYER
LI Shaoguang TANG Quanhong SONG Juyi ZHU ANG Xianglin
Cite this article: 

LI Shaoguang TANG Quanhong SONG Juyi ZHU ANG Xianglin. EFFECT OF SMALL ALLOYING ADDITIVES ON FORMATION OF Nb_3Sn LAYER. Acta Metall Sin, 1987, 23(1): 50-56.

Download:  PDF(1750KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The thickness,diffusion rate,grain size and structure of the Nb_3Sn layer prepared by modified bronze process have been examined by means of metallog- raphy,SEM,X-ray diffraction and EMPA.Both Small amount of Mg,A1 or Y added to the Cu-7at.-%Sn matrix and 1wt-% Zr added to the Nb care may ac- celerate the rate of formation and refine the grain size of the Nb_3Sn layer.The effect of addition of either 0.1—0.5 at.-% Mg to bronze or 1 wt-% Zr to Nb core is most predominante among them:The A1 added up to 1 at.-% may cause the bronze to work hardening and the specimen to premature failure under defor- mation.The structure of Nb_3Sn layer formed is of A15 type as shown by X-ray diffraction.Only trace Cu is found in Nb_3Sn layer nearby bronze,but Mg or A1 is enriched in the bronze matrix near the bronze/Nb_3Sn interface.In Nb_3Sn layer trace Mg or A1 is detected.Zr may diffuse from Nb core into bronze ma- trix in certain amount.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/50

1 Suenaga M,Klamat C,Bussiere J F.IEEE Trans Magn,1977;MAG-13:432
2 Togano Kazumasa,Asako Toshihisa,Tachikawa Kyoji.J Less-Common Met,1979;68:15-22Z
No related articles found!
No Suggested Reading articles found!