Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (1): 110-114    DOI:
Current Issue | Archive | Adv Search |
MATHEMATICAL MODEL OF BLAST FURNACE BURDENING AND PREDICTION OF ITS COKE SAVING EFFECT
WANG Huibin LU Zhongwu (Northeast Institute of Technology;Shenyang)
Cite this article: 

WANG Huibin LU Zhongwu (Northeast Institute of Technology;Shenyang). MATHEMATICAL MODEL OF BLAST FURNACE BURDENING AND PREDICTION OF ITS COKE SAVING EFFECT. Acta Metall Sin, 1987, 23(1): 110-114.

Download:  PDF(324KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The mathematical model of blast furnace burdening at low fuel rate,and regression equation of coke saving were obtained by use of optimization method. Upon this,the fuel rate,the blast furnace burden scheme at low fuel rare,the volume of Coke oven gas fed to the stove and the blast temperature obtained by burning blast furnace gas can be all predicted.Not only the mathematical model for blast furnace burdening but also its computer programs were provided.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/110

1 鞍钢炼铁厂等编著。高炉工艺计算手册.北京:冶金工业出版社,1973. 57
No related articles found!
No Suggested Reading articles found!