Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (1): 103-109    DOI:
Current Issue | Archive | Adv Search |
MATH-MODEL FOR KINETICS OF IRON ORE REDUCTION IN MOVING BED
QIN Minsheng ZHANG Yuting (Beijing University of Iron and Steer Technology)
Cite this article: 

QIN Minsheng ZHANG Yuting (Beijing University of Iron and Steer Technology). MATH-MODEL FOR KINETICS OF IRON ORE REDUCTION IN MOVING BED. Acta Metall Sin, 1987, 23(1): 103-109.

Download:  PDF(654KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The experimentally identified math-model of iron ore reduction in moving bed is developed to describe the practical process in industrial reactor.In comparison with the conventional viewpoint of kinetics,some unsimilarity among feature in solid state reduction process of iron ore in D.R.shaft furnace or in shaft of blast furnace is indicated such as:all factors influencing reduction are weakened, the reducibility of H_2 is not always superior to CO,the conventional gas heating curve would be modified and a new understanding of the reserve zone of reduc- tion process is found.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/103

1 Spitzer RH,Manning FS,philbrook W O.Trans Metall Soc AIME,242 1968;242:618
2 Yanagiya T,Yagi J,Omori Y.Ironmaking Steelmaking,6,1979;6(3) 93
3 Yagi J,Szekely J.Trans Iron Steel Jpn 1977;17:569
4 鞭严;森山昭著,蔡志鹏;谢裕生译.冶金反应工程学,科学出版社,1981
5 Ku KD,Gillis PP.Metall Trans,1981;12:111
6 谢湧堃;秦民生,金属学报,1984;20:B249:
7 Mitsuru,Tate.Paper Presented at Int.Symp.on Ironmaking,China;Wuhan,Sept.,198
No related articles found!