Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (6): 92-94    DOI:
Current Issue | Archive | Adv Search |
THE REDUCTION KINETICS OF Fe_3O_4-(xFeS·yCu_2S)-FeO-SiO_2 SYSTEM
by HUA Yixin; LIU Chunpen (Kunming Institute of Techology)
Cite this article: 

by HUA Yixin; LIU Chunpen (Kunming Institute of Techology). THE REDUCTION KINETICS OF Fe_3O_4-(xFeS·yCu_2S)-FeO-SiO_2 SYSTEM. Acta Metall Sin, 1986, 22(6): 92-94.

Download:  PDF(247KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The reduction kinetics of Fe_3O_4-(xFeS·yCu_2S)-FeO-SiO_2 system has been investigated against the slagging flux, silica granule size, mattegrade, initial magnetite content and temperature. The experimental results showed that the reaction rate increases with decreasing αFeO, matte grade and silica granule size as well as with increasing temperature. The reaction rate is controlled by the slagging reaction if the matte is saturated with Fe_3O_4, and by the reaction between S and O_2 in the melt if the matte is not saturated with Fe_3O_4. The corresponding rate equations can be expressed as: γSO_2=2.8×10~7exp(-154200/RT)W_(SiO_2)~(2/3)-α (1150-1300℃) γSO_2=3.1×10~8exp(-237900/RT)(%OFe_3O_4-b)~2(%S) (1200-1300℃) The activation energy for the reactions was found to be E_α=154.2 and E_b=237.9 kJ/mol respectively.
Received:  18 June 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I6/92

1 Liu Chunpeng (刘纯鹏); Feng Ganming (冯干明); Yan Chuanyi (来传仪); He Aiping (何蔼平), First China-USA Bilateral Metallurgical Conf., Nov. 1981, Beijing China, p. 137.
2 叶大伦,实用无机物热力学手册,冶金工业出版社,1981. p.337.
3 冶金部情报标准研究所,闪速熔炼译文集,1975,p.85.
4 Johannsen, F.; Knahl, H., Z. Erzbergbau Metallhuettenwes., 12 (1963) , 611.
5 Yazawan, A.; Kameda, M., Neutral Dissolution Between Matte and Slag Produced in System Cu_2S-FeS-FeO SiO_2, Technology Report ⅩⅠⅩ (V, № 2) , Tohoku University, Sendai, Jpn, 1955.
6 Elliott, J.F.; Mounier, M., Cand. Metall. Q., 21 (1982) , 415.6
No related articles found!
No Suggested Reading articles found!