Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (6): 46-51    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF SOLUTION STRENGTHENING OF AUSTENITE ON MARTENSITIC TRANSFORMATION IN Fe-Ni-C ALLOYS
by XU Zuyao (T.Y. Hsu); LI Jian; ZENG Zhenpeng (Shanghai Jaiotong University)
Cite this article: 

by XU Zuyao (T.Y. Hsu); LI Jian; ZENG Zhenpeng (Shanghai Jaiotong University). EFFECT OF SOLUTION STRENGTHENING OF AUSTENITE ON MARTENSITIC TRANSFORMATION IN Fe-Ni-C ALLOYS. Acta Metall Sin, 1986, 22(6): 46-51.

Download:  PDF(518KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The M_s temperature and the yield strength of austenite have been measured for 5 various Fe-Ni-C alloys. The solution strengthening of austenite at M_s temperature can be expressed as: σ_(0·2)(M_s)=25.9+3410x_c+567x_(Ni) MPa, and the effect of C and Ni content on M_s temperature can be shown as: M_s (K)=829-8650x_c-1766x_(Ni·) The linear relationship between M_s temperature and σ_(0·2)(M_s) can be written as: σ(0·2)(M_s)=210-0.323M_s(℃) MPa. These equations indicate that the solution strengthening of austenite at M_s temperature acts as the resistance of martensitic transformation and the linear relation exists not only between σ0·2(M_s) and M_s, but also σ_(0·2)(M_s) and the driving force for martensitic transformation. Since the substructure of martensite depends on the Ni and C content in alloys, a schematic sketch showing the effect of σ_(0·2)(M_s) on the morphology of martensite in Fe-Ni-C alloys is developed through the work of Magee and Davies. Based on this view, the relationship between σ_(0·2)(M_s) and the critical resolved shear stress may be sketched which interpret the formation of dislocation and twinned martensite.
Received:  18 June 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I6/46

1 Schiel, E., Z. Anorg. Chem., 207(1932) , 21.
2 Kelly, P.M.; Nutting, J., J. Iron Steel Inst., 197(1961) , 199.
3 Philibert, J., C.R. Hebd. Seances Acad. Sci., 240(1955) , 190.
4 Crussard, C., The Mechanism of Phase Transformations in Metals, Inst. of Metals Monogragh and Report 1955, Ser. 18, p. 309.
5 Sastri, A.S.; West, D. R. F., J. Iron Steel Inst., 203(1965) , 138.
6 Ankara, A., J. Iron Steel Inst., 208(1970) , 819.
7 Woehrle, H.R.; Clough, W.R.; Ansell, G.S., ASM Trans. Q., 59(1966) , 784.
8 Donaehie, S. J.; Ansell, G.S., Metall Trans., 6A(1975) , 1863.
9 Umemoto, M.; Owen, W.S., Metall Trans., 5(1974) , 2041.
10 Nichol, T.J.; Judd, G.; Ansell, G.S., Metall. Trans., 8A(1977) , 1877.
11 Brofman, P.J.; Ansell, G.S., Metall. Trans., 14A(1983) , 1929.
12 Hsu, T.Y. (徐祖耀); Yah Linfah (颜林发), J. Mater. Sci., 18(1983) , 3213.
13 徐祖耀;颜林发,金属学报,20(1984) , A143.
14 Ansell, G.S.; Brofman, P.J.; Nichol, T.J.; Judd, G., ICOMAT-79, Cambridge, Massachusetts, 1979, p. 350.
15 Hsu, T.Y. (徐祖耀); yan, Linfah (颜林发), Metalligraphy, 17(1984) , 397.
16 Breinan, E.M.; Ansell, G.S., Metall. Trans., 1(1970) , 1513.
17 Yeo, R.B.G., Trans. Metall Soc.AIME, 227(1963) , 884.
18 Wilson, E.A., Met.Sci., 18(1984) , 471.
19 徐祖耀,马氏体相变与马氏体,科学出版社,北京,1980. p.407.
20 Maxwell, P. C.; Goldberg, A.; Shyne, J. C., Metall. Trans., 5(1974) , 1305.
21 徐祖耀,金属学报,15(1979) ,329。
22 徐祖耀,金属学报,16(1980) ,420。
23 Hsu, T.Y. (徐祖耀), J. Mater. Sci., 20(1985) , 23.
24 Rao, M.M.; Russell, R.J.; Winchell, P.G., Trans. Metall. Soc. AIME, 239(1967) , 634.
25 Hornbogen, E., Physical Metallurgy, Ed. Cehn, R.W., North-Holland, 1970, Chap. 10a.
26 Magee, C.L.; Davies, R.G., Acta Metall., 19(1971) , 345.
27 Westlake, D.G., Deformation Twinning, Ed. Reed-Hill, R.E., Gordon and Breach,New York. 1964, p. 29.
28 Venables, J.A., Deformation Twinning, Ed. Reed-Hill, R.E., Gordon and Breach, New York, 1964, p. 77.V
No related articles found!