EFFECT OF INTERCRITICAL HEAT TREATMENT ON MICROSTRUCTURE OF MARTENSITIC STEEL 12Ni4CrMo
by SONG Chengyi; SHEN Yunhua; ZHANG Guangzhong; WU Guangda (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing)
Cite this article: 

by SONG Chengyi; SHEN Yunhua; ZHANG Guangzhong; WU Guangda (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). EFFECT OF INTERCRITICAL HEAT TREATMENT ON MICROSTRUCTURE OF MARTENSITIC STEEL 12Ni4CrMo. Acta Metall Sin, 1986, 22(6): 36-40.

Download:  PDF(1943KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  TEM and SEM studies were carried out on the low carbon martensitic steel 12Ni4CrMo undergone intercritical heat treatment. The influence of the quenching temperature between A_(c_1)—A_(c_3) on the morphology, phase constitution as well as -196℃ CVN toughness were analyzed in comparison with the steel conventionally treated. It is suggested that the effective grain refinement, the configuration of zigzag prior austenite grain boundary and the suitable substructure are the important microstructural characteristics of the intercritically treated steel. These seem to be the main factors contributing to the optimum toughness.
Received:  18 June 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I6/36

1 Kim, J.I.; Syn, C.K.; Morris, J.W. Jr., Metall. Trans., 14A(1983) , 93.
2 Matsuda, S.; Inoue, T.; Ogasawara, M., Trans. Jpn. Inst. Met., 9(1968) , 343.
3 大谷泰夫;寺崎富文长;邦武立郎,铁钢,58(1972) ,434。
No related articles found!
No Suggested Reading articles found!