PHASE EQUILIBRIUM AND HYDROGEN ABSORPTION OF Ni-Fe-16.7at.-%La SYSTEM
by WANG Chaoguo; DAI Shouyu (Institute of Physics; Academia Sinica; Beijing)
Cite this article: 

by WANG Chaoguo; DAI Shouyu (Institute of Physics; Academia Sinica; Beijing). PHASE EQUILIBRIUM AND HYDROGEN ABSORPTION OF Ni-Fe-16.7at.-%La SYSTEM. Acta Metall Sin, 1986, 22(6): 110-113.

Download:  PDF(330KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The phase equilibrium relationship of the Ni-Fe-16.7 at.-%La system has been investigated by means of X-ray diffraction and DTA. The Ni-riched region has a peritectic reaction. A new hexagonal intermetallic compound LaNi_3Fe_2is identified. The absorption and desorption of hydrogen by the system and by this new compound were also examined.
Received:  18 June 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I6/110

1 戴守愚;王朝果;滕晨明;肖南;齐上雪,金属学报,18(1982) ,599.
2 Sandrock, G.D., Hydrogen Energy System, Proc. 2nd World Hydrogen Energy Conf., Switzrland, Zurich, Aug., 1978, Vol. 3, Eds. Veziroglu, T.N.; Seifrits, W., Pergamon, Oxford, 1978, p. 1625.
3 Van Mal, H.H.; Buschow, K.H.J.; Miedema, A.R., J. Less-Common Met., 35 (1974) , 65.
4 三沢俊平;能町暁彦;矢岛聖使;管原英夫,日本金属学会誌,43(1979) ,104.
5 Dwight, A.E., Rare Earths in Modern Science and Technology, Proc. 13th Rare earth Res. Conf, (1977) , Eds. MaCarthy, G.J.; Rhyne, J.J., Plenum Press, New York, 1978, p. 325.
6 梁敬魁;王朝果,金属学报,18(1982) .592.
7 Haefling, J,; Daane, A.H., The Eare Earth, Eds. Spedding, F.H.; Daane, A.H., Wiley, New York, 1961, p. 280.
8 庄应烘;荣国器;唐晓峰,中国稀土学报,1(1983) ,58.Q
No related articles found!
No Suggested Reading articles found!