Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (5): 89-154    DOI:
Current Issue | Archive | Adv Search |
TEM STUDY OF AUSTENITE FORMATION IN A LOW CARBON STEEL
YANG Dezhuang (Harbin Institute of Technology)
Cite this article: 

YANG Dezhuang (Harbin Institute of Technology). TEM STUDY OF AUSTENITE FORMATION IN A LOW CARBON STEEL. Acta Metall Sin, 1986, 22(5): 89-154.

Download:  PDF(2832KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The normalized and normalized plus cold-rolled structures and their effects on the formation of austenite in 0.08C-1.5Mn steel were examined by TEM. It was shown that during intercritical annealing, the austenite formation was accompanied by spheroidization of cementite in the initially normalized structure, a result attributed to the existence of more dislocation in ferrite and degenerated pearlite containing many changes in spacing and interruption in lamellar morphology in the normalized condition. The austenite nucleated not only at the cementite particles located at the triple points and faces of ferrite grain boundaries, but also at the interfaces of ferrite and cementite which was within ferrite matrix. Due to the effect of cold rolling, the lamellar cementite in the cold-rolled structure was distorted severely and even fragmented. Also, a great amount of dislocations were introduced into the ferrite matrix. These effects of the cold rolling accelerated the spheroidization of cementire and enhanced the possibility that the austenite formed within ferrite grains during intercritical annealing. The relationship between austenite formation and cementite spheroidization and the possible sites of austenite nucleation were discussed.
Received:  18 May 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I5/89

1 沈显璞;雷廷权,金属热处理学报,2(1981) .№1. 62;№2. 65.
2 Zwell, L.; Gorman, L.A.; Weissmann, S., ASM Trans. Q., 59(1966) , 491.
3 Nakagawa, Y.G.; Weatherly, G.C., Metall. Trans., 3A (1972) , 3223.
4 Speich, G.R.; Demarest, V.A.; Miller, R.L., Metall. Trans., 12A(1981) , 1419.'