AN INSCRIPTION ON THE MODEL OF THE ANCIENT COMPASS——SI NAN |
by DAI Lizhi (Tai Li-chi) (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
|
Cite this article:
by DAI Lizhi (Tai Li-chi) (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). AN INSCRIPTION ON THE MODEL OF THE ANCIENT COMPASS——SI NAN. Acta Metall Sin, 1986, 22(4): 83-85.