Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (4): 80-82    DOI:
Current Issue | Archive | Adv Search |
TRANSITION OF GRAPHITE MORPHOLOGY IN CAST IRON AND ITS GROWTH KINETICS
by YAO Xin; DING Shaolang; WU Xueming; XU Zhaohua; LI Songchun; WANG Wuxian (Shanghai Jiaotong University)
Cite this article: 

by YAO Xin; DING Shaolang; WU Xueming; XU Zhaohua; LI Songchun; WANG Wuxian (Shanghai Jiaotong University). TRANSITION OF GRAPHITE MORPHOLOGY IN CAST IRON AND ITS GROWTH KINETICS. Acta Metall Sin, 1986, 22(4): 80-82.

Download:  PDF(1255KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of solidification rate, modifying agent added and fading on the morphology of graphite were investigated by means of the technique of the liquid metal cooling directional solidification. The model of growth of graphite crystal was also proposed.
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/80

1 Liu, P.C.; Loper, C.R., Trans. Ant Foundrymen's Soc., 88 (1980) , 97-118.
2 姚忻;丁少兰,金属科学与工艺,(1985) ,№3,50.
No related articles found!