ACTIVITY OF Ce_2O_3 IN LIQUID SLAGS OF Ce_2O_3-CaO-CaF_2 SYSTEM
by WANG Changzhen; YE Shuqing (Northeast Institute of Technology; Shenyang); HU Yingnian; DU Qisheng (Nei Monggol Institute of Metallic Materials)
Cite this article: 

by WANG Changzhen; YE Shuqing (Northeast Institute of Technology; Shenyang); HU Yingnian; DU Qisheng (Nei Monggol Institute of Metallic Materials). ACTIVITY OF Ce_2O_3 IN LIQUID SLAGS OF Ce_2O_3-CaO-CaF_2 SYSTEM. Acta Metall Sin, 1986, 22(4): 77-79.

Download:  PDF(217KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The liquid boundary of the slags of Ce_2O_3-CaO-CaF_2 system and the iso-activity lines for Ce_2O_3 and CeO_2 are given from experimental determination of the activity of Ce_2O_3 by equilibrating the slag with Sn in a graphite crucible under an atmosphere of CO at 1600℃. The activity of Ce_2O_3 in the slags containing certain CeO_2 or CaO, increases with the increase of concentration of CaO or CeO_2 respectively. The transition of CeO_2 to Ce_2O_3 under the condition of high temperature and low oxygen partial pressure was also discussed by thermodynamical analysis.
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/77

1 邹元燨;赵彭年;曹兆民,金属学报,6(1963) ,121.
2 Chou Yuan-hsi(邹元燨),Chow Ji-cheng(周继程);Chao Peng-nian(赵彭年),Sci.Sinica,12 (1963) .1249.
3 王常珍,邹元燨,金属学报,16(1980) ,190.
4 王常珍,杨代银,金属学报,15(1979) .433.
5 Iwasaki, B.; Katsura, T., Bull. Chem. Soc. Jpn., 44 (1971) , 1297.
6 Bevan, D.J.; Kordis, J., J.Inorg. Nucl. Chem., 26 (1964) , 1509.
7 Fruehan, R.J., Metall, Trans., 10B (1979) , 143.
8 #1
No related articles found!
No Suggested Reading articles found!