| COMPLETE INTEGRATION OF GIBBS-DUHEM EQUATION ALONG PHASE BOUNDARIES IN MULTICOMPONENT SYSTEMS |
| by FANG Zheng (Central South University of Technology; Changsha) |
|
Cite this article:
by FANG Zheng (Central South University of Technology; Changsha). COMPLETE INTEGRATION OF GIBBS-DUHEM EQUATION ALONG PHASE BOUNDARIES IN MULTICOMPONENT SYSTEMS. Acta Metall Sin, 1986, 22(4): 74-76.
|
|
|
Abstract A new method has been developed to solve the problem of complete integration of the Gibbs-Duhem equation along phase boundaries in a c-component and c-1-phase system. Two variables, (△_1)_(1i)=D_i/D_i and (△_i)_(1i)=D_i/D_(1i), are introduced into the Gibbs-Duhem equation for multicomponent systems. And the function φ suggested by Chou for use in a miscibility gap of ternary systems is extended. Activities of component f on whole phase boundaries may be calculated from the known experimental values of a_1 by means of the modified Gibbs-Duhem equation without integral difficulties.
|
|
Received: 18 April 1986
|
| 1 Gokcen. N.A.; Chang, E.T., J. Electrochem. Soc., 119 (1972) , 876.
2 周国治.中国科学,3(1978) .312.
3 Chou K-C; Elliott, J.F., Chemical Metallurgy-A Tribute to Carl Wagner, TMS-AIME, 1981, p. 195. |