EFFECT OF GRAPHITE NODULES ON FRACTURE TOUGHNESS OF NODULAR CAST IRON
by LI Zhonghua; LIU Ai; ZHOU Huijiu; KUANG Zhenbang (Xi'an Jiaotong University)
Cite this article: 

by LI Zhonghua; LIU Ai; ZHOU Huijiu; KUANG Zhenbang (Xi'an Jiaotong University). EFFECT OF GRAPHITE NODULES ON FRACTURE TOUGHNESS OF NODULAR CAST IRON. Acta Metall Sin, 1986, 22(4): 43-55.

Download:  PDF(934KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A model with local composite structure is used to simulate the microstructure of nodular cast iron at a small crack tip region of the three-point bending specimen This model allows to get a solution close enough approaching the solution of a real material The J-integral in a material with composite structure is discussed It is found that the fracture toughness of nodular cast iron is practically the fracture toughness of steel with holes The effects of the graphite shape, size, volume fraction etc. on the stress intensity factor and fracture toughness of nodular cast iron are also examined. In the finite element calculation, the elastoplastic increment theory with finite deformation has been used The calculated results agree well with experimental data
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/43

1 无锡柴油机厂等,球铁,(1978) ,№2,8.
2 徐驰;余瑞珍,金属学报,14(1978) ,40.
3 Ruff, G.F.; Doshi, B.K., Mod. Cast., 70 (1980) ,№ 7, 70.
4 Loper, C. R., Trans. Am. Foundrymen's Soc., 83 (1975) , 245.
5 周承倜,胡义祥,第二届全国断裂力学会议宣读论文,1980.
6 嵇醒,殷家驹,西安交通大学学报,(1979) ,№3,61.
7 Memeeking, R.M.; Rice, J.R., Int. J. Solids Struct., 11 (1975) , № 11, 601.
8 Hofmeister, L.D.; Greenbaum, G.A.; Evensen, D.A., AIAA J., 9 (1971) , 1248.
9 Kuang Zhenbang, Eng. Fract. Mech., 19 (1984) , 1161.
No related articles found!
No Suggested Reading articles found!