Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (4): 32-148    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF ADDITIVE Sr OR Sb ON MODIFICATION OF Al-Si ALLOYS
by HUANG Liangyu; WANG Yucong; ZHAI Chunquan; DING Wenjiang (Department of Materials Science and Engineering; Shanghai Jiaotong University)
Cite this article: 

by HUANG Liangyu; WANG Yucong; ZHAI Chunquan; DING Wenjiang (Department of Materials Science and Engineering; Shanghai Jiaotong University). INFLUENCE OF ADDITIVE Sr OR Sb ON MODIFICATION OF Al-Si ALLOYS. Acta Metall Sin, 1986, 22(4): 32-148.

Download:  PDF(3187KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The modification of five Al-Si alloys of different purity and composition with 9—14 wt-% Si at various cooling rates influenced by an additive Sr or Sb has been investigated in detail by means of SEM, EPMA, etc. The microstructural nomograph of these Al-Si alloys is constructed to provide for the selection of optimum addition of Sr or Sb in production practice Experimental results indicate a threshold of Sr content in Al-Si alloy modification, over it, the structure of Al-Si alloy may be completely modified even at quite slow cooling rate down to 4.5℃/min. The threshold increases with the decrease of cooling rate Both Sr and Sb can retard the initiation of Si precipitation, but differ in the influence on the growth form of eutectic Si
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/32

1 Hess, P.D., Trans. Am. Foundrymen's Soc., 83 (1975) , 87.
2 Leandro, L.M.; Serafin, F.R., 43rd International Foundry Congress Paper, 1976, Bucharest Rumania.
3 Davami, P.; Ghafelehbashi, M., Br. Foundryman, 72 (1979) ,№ 1, 4.
4 French Paper: Trans. Am. Foundrymen's Soc., 86 (1978) , 549.
5 Jenkinson, D.C.; Hogan, L.M., J. Cryst. Growth. 28 (1975) , 171.
6 黄良余;翟春泉;林凡,铝硅合金新的变质方法,第三届全国铸造年会论文,1978.
7 津村善重;榊原秋策;璺田勝(氵郎),石川正武,轻金属,30(1980) ,239.
8 朱培钺,陈熙琛,贾均,张宝书;刘贤功,哈尔滨工业大学科学研究报告,第155期,1979.
9 Verhoeren,J.D.,物理冶金学基础,卢光熙;赵子伟译,上海科学技术出版社,1980,p.152.J
No related articles found!
No Suggested Reading articles found!