IMPROVING CONTACT FATIGUE STRENGTH OF CARBONITRIDING GEAR STEEL 25MnTiBR WITH RETAINED AUSTENITE
by JIANG Bingyuan; SHAO Eryu (Luoyang Institute of Technology)
Cite this article: 

by JIANG Bingyuan; SHAO Eryu (Luoyang Institute of Technology). IMPROVING CONTACT FATIGUE STRENGTH OF CARBONITRIDING GEAR STEEL 25MnTiBR WITH RETAINED AUSTENITE. Acta Metall Sin, 1986, 22(4): 19-25.

Download:  PDF(540KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A study was made of the behaviour of retained austenite to improve the contact fatigue strength of the carbonitriding gear steel 25MnTiBR by means of the contact fatigue test, the fracture mechanics analysis of spalling on contact surface and the energy estimation of crack tip plastic zone The retained austenite deformation induces the martensite transformation, which absorbs energy more than one half of the strain energy of material It may retard the propagation of fatigue cracking and may improve the contact fatigue strength of the carbonitriding steel 25MnTiBR with retained austenite The proper material together with a reasonable technique chosen for production practice may be available to obtain more and not very stable retained austenite in the surface layer of the gear, especially, it may improve the gears under heavy load.
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/19

1 邵尔玉;陈菁;王长生,金属热处理学报,2(1981) ,№1. 43.
2 邵尔玉;吴逸贵;顾进立,洛阳农学院学报,(1981) ,№1,99.
3 肖纪美,金属的韧性与韧化,上海科技出版社,1980,p.337.
4 邵尔玉;姜秉元;王长生,金属热处理,(1983) .№3,30.
5 徐祖耀,马氏体相变与马氏体,科学出版社,1980,p.381.
6 田村今男,钢的组织转变译文,姚忠凯译,机械工业出版社,1980,p.289.X
No related articles found!
No Suggested Reading articles found!