MICRODISTRIBUTION OF Ce IN CERTAIN STEELS AND Fe-Cr-Al ALLOY
by HAN Qiyong; HUO Chengzhang; ZHONG Weizhen; PENG Ming; (Beijing University of Iron and Steel Technology)
Cite this article: 

by HAN Qiyong; HUO Chengzhang; ZHONG Weizhen; PENG Ming; (Beijing University of Iron and Steel Technology). MICRODISTRIBUTION OF Ce IN CERTAIN STEELS AND Fe-Cr-Al ALLOY. Acta Metall Sin, 1986, 22(4): 15-146.

Download:  PDF(2879KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The method for the determination of alloyed amounts of rare earth metals in steels developed previously by the authors was verified to be appropr ate Using this method, the alloyed amount of Ce in steels 16Mn, 25MnTiB, Cr24Ni7Si2N and Fe-Cr-A1 alloy has been analysed The microautoradiographs show that the alloyed Ce distributed among the pearlite is more than that among the ferrite in 16Mn or 25MnTiB steel. An enrichment of Ce was obviously observed by autoradiography to be segregated along the grain and dendrite boundaries in Fe-Cr-Al alloy or Cr24Ni7Si2N when the Ce content is notl ow The microscopic inhomogeneity of Ce distribution is presented among different grains of the Fe-Cr-Al alloy.
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/15

1 Han Qiyong; Wu Weijiang; Fang Keming; Huo Chengzhang; Zhou Xiaolong, Proc. of Sino-Jpn Symp. on Iron and Steel, First Symp. on Steelmaking, Beijing, 1981, p, 25;钢铁, 16 (1982) , № 2, 1.
2 韩其勇,吴卫江,方克明,张保军,谢德义;裴丽侠,金属学报,15(1979) ,1.
3 zhong Weishen(钟伟珍),Han Qiyong(韩其勇),Huo Chengzhang(霍成章); New Frontiers in Rare Earth Science and Application Vol.Ⅱ, Proc. of the Int. Conf. on Rare Earth Development and Applications, Beijing. China, Sep., 1985, Eds. Xu Ghangxian; Xiao jimei; Science Press, Beijing, 1985, p.10-14.
4 Wilson, W.G.; Wells, R.G., Met. Progr., 104 (1973) , 7, 75.
5 #12
6 #12
7 #12
8 #12
9 川村和郎;渡辺四郎;鈴木節雄,铁钢,61(1975) ,2784.
10 Golightly, F.A.; Stott, F.H.; Wood, G.C., Oxid. Met., 10 (1976) , № 3. 163.
11 骆继勋,银耀德,林生昆,赵齐,王俭,金属学报,13(1977) ,263.
No related articles found!
No Suggested Reading articles found!