MICROHARDNESS AND STRUCTURAL RELAXATION IN AMORPHOUS Zr-Co AND Zr-Ni ALLOYS
by ZHANG Qirui (Department of Physics; University of Science and Technology of China; Hefei); FREYHARDT Herbert C. (Institut fur Metallphysik; Universitat Gottingen; FRG)
Cite this article: 

by ZHANG Qirui (Department of Physics; University of Science and Technology of China; Hefei); FREYHARDT Herbert C. (Institut fur Metallphysik; Universitat Gottingen; FRG). MICROHARDNESS AND STRUCTURAL RELAXATION IN AMORPHOUS Zr-Co AND Zr-Ni ALLOYS. Acta Metall Sin, 1986, 22(4): 125-127.

Download:  PDF(288KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The dependence of microhardness on the Co or Ni concentration has been measured for amorphous Zr_(100-x)M_x (M=Co, 22 x≤53.4; M=Ni, 24.1 x≤63.8) alloys. It is shown that the microhardness increases systematically upon increasing the concentration of Co or Ni. The effect of structural relaxation on the microhardness has been investigated for Zr_(78) Co_(22) and Zr_(75.9)Ni_(24.1). The microhardness exihibits a minimum and, then, increases slowly during isothermal annealing at 250℃. For isochronous annealing at differe nt temperature the microhardness increases very sharply when the crystallization temperature is approached. Complementary experimental results of DSC, resistivity, superconducting-critical-temperature and X-ray-diffraction measurements are used for an analysis of the phenomena occurring during structural relaxation and crystallization.
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/125

1 Chen, H.C., J. Appl. phys., 49 (1978) , 3289.
2 Chen, H.C.; Leamy, H.J.; Barmatz, M., J. Non-Cryst. Solids, 5 (1971) , 444.
3 Berry, B.S.; Pritchet, W.C., J. Appl. Phys., 44 (1973) , 3122.
4 Williams, R.S.; Egami, T., IEEE Trans. Magn., MAG-12 (1976) , 927.
5 Masumoto, T., Sci Rep. Res. Inst., Tohoku Univ., A26 (1977) , 426.
6 Chen, H.S.; Lo, C.C., Proc. 2nd Int. Conf. on. Rapidly Quenched Metals, Massachusetts Institute of Technology Press, Cambridge, Mass, 1976, p. 413.
7 张其瑞;Freyhardt,H.C.,低温物理,6(1984) ,176.
8 Ray, R.; Hasegawa, R.; Chou, C.P.; Davis, L.A., Scr. Metall., 11 (1977) , 973.
No related articles found!
No Suggested Reading articles found!