LOW TEMPERATURE RESISTIVITY ANOMALY FOR AMORPHOUS (Fe_(1-x)V_x))_(84)B_(16) ALLOYS
by CHEN Jinchang (Beijing Teachers' College); ZHAN Wenshan; SHEN Baogen; ZHAO Jiangao (Institute of Physics; Academia Sinica; Beijing); SI Hong (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing)
Cite this article: 

by CHEN Jinchang (Beijing Teachers' College); ZHAN Wenshan; SHEN Baogen; ZHAO Jiangao (Institute of Physics; Academia Sinica; Beijing); SI Hong (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). LOW TEMPERATURE RESISTIVITY ANOMALY FOR AMORPHOUS (Fe_(1-x)V_x))_(84)B_(16) ALLOYS. Acta Metall Sin, 1986, 22(4): 121-124.

Download:  PDF(278KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The electrical resistivity of amorphous (Fe_(1-x)V_x)_(84)B_(16) (x=0—0.1) alloys as a function of temperature between 4.2—300 K has been studied. It was shown that the resistivity minima over the whole concentration range seem to be presented; below T_(min) it showing maxima at x=0.02—0.1; over T_(min), as a T~2 temperature dependence. The low temperature resistivity anomaly is likely to originate from Kondo-like effect, RKKY interaction and localized spin-fluctuation scattering.
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/121

1 詹文山;沈保根;郭慧群,低温物理,5(1983) ,№2,91.
2 沈保根;詹文山;章志英;吴宗林,金属学报,20(1984) ,B164.
3 陈金昌;詹文山;沈保根;赵见高,乐观,物理学报,35(1986) ,25
4 Chan, W.S.; Shen, B.G.; Lo, H.Y.; Yu, B.L., Proc. 4th Int. Conf. on Rapidly Quenched Metals, (Sendai, 1981) , Eds. Masumoto, T.; Suzuki, K., JIM, 1982, p. 1137.
5 汪仲诚;刘福绥,物理学报,32(1983) ,33.
6 李正中;胡筱欣;王金才,物理学报,34(1985) ,145.
No related articles found!
No Suggested Reading articles found!