Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (4): 11-144    DOI:
Current Issue | Archive | Adv Search |
THE M-A STRUCTURE AND BAINITE IN ULTRA HIGH STRENGTH LOW ALLOY STEELS
by ZHONG Bingwen; SONG Yuwen (Institute of Aeronautical Materials; Beijing)
Cite this article: 

by ZHONG Bingwen; SONG Yuwen (Institute of Aeronautical Materials; Beijing). THE M-A STRUCTURE AND BAINITE IN ULTRA HIGH STRENGTH LOW ALLOY STEELS. Acta Metall Sin, 1986, 22(4): 11-144.

Download:  PDF(2045KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An observation under TEM was made of the (M-A) structure and "bamboo shaped" bainite in the isothermally quenched ultra high strength steels containing Si after the isothermal transformation The retained austenite in the isothermal structure of bainite region at temperature≥300℃ is often found in the M-A and "bamboo shaped" bainite In the bainite formed isothermally at 180, 300, 320 and 420℃, the ε-carbide is observed. The type of carbide in decomposition products is related to the distribution and morphology of retained austenite. The ε-carbide may precipitate along the austenite side of martensite/austenite boundary.
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/11

1 Thomas. G., Metall, Trans., 9A (1978) , 439.
2 Marasimha Rao, B.V.; Thomas, G., Metall. Trans., 11A (1980) , 441.
3 73 (1950) , 1161.
4 Huang, D.-H.; Thomas, G., Metall. Trans., 8A (1977) , 1661.
5 Jack, K.H., J. Iron Steel Inst., 169 (1951) , 26.
6 Sarikaya, M.; Thingan, A, K.; Thomas, G., Metall Trans., 14A (1983) , 1121.
7 Aaronson, H.I.; Plichta, M.R.; Franti, G.W.; Russell, K.L., Metall. Trans., 9A (1978) , 363.
8 李春志,物理学报,28(1979) ,314.?
No related articles found!